metalresearcher - 1-10-2016 at 22:48
I have some CaO and want to make firebricks in which I can deploy an electric arc with a 150A DC welder.
Any other refractory melts and vaporizes (yes, I know, CaO too, but slower due to higher mp, so they last longer).
Is there a binder (clay ?) with which I can make small bricks from CaO powder ?
Jstuyfzand - 2-10-2016 at 01:28
You would be better off buying some proper bricks and carving a reactor from it, a la Grant Thompson.