I'd take blogfast's advice and try to extract the stuff with toluene or some other nonpolar solvent. At the same time, I don't really see what organic
impurities could exist from reacting the metal with nitric acid.
Then dissolve the crude nitrate in water and precipitate the hydroxide with ammonia. I highly recommend making the acetate instead if you want to grow
crystals, as it's far less hygroscopic - just dissolve the hydroxide in acetic acid and crystallize it. If there's a higher praseodymium oxide
present, it'll remain as a solid and can be filtered off. |