I received the 10%Pd/C gratis from Billy in LaJolla a few days ago as promised (see my post in Preparation of Succinic Acid). As
suggested by Dr Bob, today I tested its activity using methanol. Then I tested it using propane. The results were negative. My son made three short
movies of this testing. So, from the studios of Mr Ardipithicus, here they are:
https://youtu.be/enEykN7nbsQ
https://youtu.be/PSTSCmskPd0
https://youtu.be/lCDD7KWRaB4
As indicated in the last movie, if you have any suggestions for further tests, or corrections to my tests, please let me know.
[Edited on 14-10-2016 by Magpie]: reposted last video - seems to work OK now.
[Edited on 14-10-2016 by Magpie] |