mahy - 2-7-2016 at 00:29
Hi
How can I deposit carbon black from water solution with lingo sulphonate??
hissingnoise - 2-7-2016 at 03:35
Very messily, I'd imagine ─ and I must assume you mean lignosulphonates?
Welcome to scimad.
mahy - 2-7-2016 at 21:29
actually i am looking for accumulation agent for carbon black.
mahy - 2-7-2016 at 22:05
Can i remove carbon black by filtration??
hissingnoise - 3-7-2016 at 05:37
Practically all particulate matter can be filtered, but without the details of what you're actually doing it's hard to advise!
mahy - 3-7-2016 at 21:03
i have a Aqueous solution of carbon black and lignosulphonate and i want to measure percent of carbon black and lignosulphnate.
Carbon black is insoluble in water and lignosulphonate is soluble, but carbon black doesn't deposit and it's particles are too small for filtration.
So i am looking for coagulant aid to can filter it.
Fleaker - 4-7-2016 at 06:35
Try cellite?