Sciencemadness Discussion Board

Gold Recovery with Salt Vinegar Bleach peroxide - VIDEO

kadriver - 16-10-2015 at 11:35

Here is all three parts of the video showing how the foils are lifted off the fingers. These videos are buried in another thread so I hope this is not counted as a double post;

Part 1, using salt, vinegar and hydrogen peroxide to lift the foils from trimmed circuit card fingers.

https://youtu.be/ouYW_7-Njbs

Part 2, recovering the lifted foils for refining then dissolving the gold foils in salt and vinegar with bleach

https://youtu.be/TUxJ0YhATxM

Part 3, precipitating the pure gold with vitamin C

https://youtu.be/CAhh6p4E6-I

kadriver

aga - 16-10-2015 at 12:08

Useful precis of the process deltaH came up with.

It is a bit like Spam, as it could easily go in the main thread.

Much easier to Find like this though.

[Edited on 16-10-2015 by aga]

cyanureeves - 16-10-2015 at 16:58

kadriver you know that pungent smell you get when precipitating with smb?well what does vitamin c smell like?

kadriver - 16-10-2015 at 18:41

I didn't smell anything because it was in my fume hood. I'm curious though. Maybe I'll do it outside to see what kind of odor it produces.