they can run at the same temperatue were Polystyrene decompose back into styrene
blend the polystyrene add some water so the water take the place of the air
that is in the reaction vessel
and heat the hell out of the reaction vessel for an hour i guess
stopping the heating, lets it cool down to room temp, look into the vessel to see if there any liquid that look like styrene
sound good ? Oscilllator - 17-8-2015 at 17:35
Perhaps you should look to see if anyone else has tried depolymerizing styrene. If you do, you will find a number of resources on the subject
including a video detailing the process made by a member of this forum.UC235 - 17-8-2015 at 17:52
I have a writeup in prepublication that I think should be quite sufficient.Oscilllator - 17-8-2015 at 17:57