SAM4CH - 11-12-2005 at 13:50
How can I get pure Di Butyl Phthalate from nail polish?!
ordenblitz - 11-12-2005 at 16:59
It would take a lot of nail polish as Phthalates are added in small percentages as a plasticizer for the nitrocellulose lacquer. Since nail polish is
intended to be shiny and hard, and is put on a fairly inflexible substrate (fingernails) very little plasticizer is typically used.