I forgot what page I was looking at, but Divinylbenzene + Styrene + a photointiator seems to be a reliable polymer blend that will form a chemically
resistant polymer when activated. Divnylbenzene behaves as a crosslinking agent.
Unless I'm mistaken, isn't Styrofoam polystyrene? Isn't styrene the monomer and polystyrene the polymer? Styrene is a liquid, polystyrene a solid.
Styrofoam easily dissolves in solvents like acetone.