From Benjamin-Moore paints webbie:
Super Spec HP Epoxy
Two component, catalyzed epoxy coatings provide excellent chemical resistance, good solvent resistance, good acid resistance, and very good abrasian
resistance. By adjusting the epoxy resin, pigments, and additives they can produced as primers or finish coats with a wide variety of gloss levels.
Two component epoxies cure by solvent evaporation plus chemical curing when the two components are combined. |