I decided to give the whole "precious metals from computers" thing a try. The one thing I'm worried about is separating the metals from one another.
I'm aware that palladium dissolves slowly in some acids. This then worries me that I will lose it during the removal of less valuable metals, but if
it is slow enough I can't lose that much. I figure if that is the case, after precipitating the metals I could treat it with nitric or sulfuric acid
and that would get the palladium out on it's own. Does anyone have any ideas on what else I could do?
hyfalcon - 29-4-2014 at 18:35
You have to register to read this forum but it's well worth the trouble.
http://goldrefiningforum.com/phpBB3/viewforum.php?f=34
Brain&Force - 29-4-2014 at 18:59
Also try the YouTube channel "indeeditdoes" for the practical side of gold refining. (Recommended by NurdRage)