A suggestion may be to heat the tube (so effectively just the argon gas) slightly upstream of the boat and not have the flame directly below the
boat, thereby having hot Ar heating the boat and avoiding a hot spot on the boat surface underneath that fuses the product locally.
[Edited on 13-4-2014 by deltaH] |