vmelkon - 7-4-2014 at 11:47
I have noticed that when I get prescription drugs, it is now in polypropylene instead of polystyrene. This is in Quebec, Canada.
Is it that way in your area as well?
plante1999 - 7-4-2014 at 11:49
Yes, it is the same here in Quebec city, Quebec Canada.
jwpa17 - 7-4-2014 at 17:01
I've noticed it here in western Pennsylvania, USA, as well. Also that more foods are coming in PETE rather than polystyrene. Not sure why.