Sciencemadness Discussion Board

regenerate tlc plates?

soma - 25-10-2013 at 19:53

Is there a way to regenerate plastic backed silica gel tlc plates?

Thanks.

confused - 25-10-2013 at 22:40

scrape off the silica and spread the silica el and bake it?

although it'll probably be easier with glass backed plates

this might help
http://www.sciencemadness.org/talk/viewthread.php?tid=12350

[Edited on 26-10-2013 by confused]

PHILOU Zrealone - 26-10-2013 at 01:53

Also several washes with a "pure solvent" or different solvents or a solvent mixe might help to regenerate the plates....

But everything depends on what you have put onto it for chromatography and its affinity for the plate.

Some spots remains very attracted by the silica and then it is useless...only very agressive chems detrimental to the silica would take those off.