wish i had a kraken!!! - 22-3-2012 at 13:41
Hi everyone , is there anybody who knows how I can synthesis KClO4???
Help me with it please.
[Edited on 22-3-2012 by wish i had a kraken!!!![:)](./images/smilies/smile.gif)
[Edited on 22-3-2012 by wish i had a kraken!!!]
friendly suggestions
Fleaker - 22-3-2012 at 13:44
You can start with the search engine.
![Screen Shot 2012-03-22 at 5.42.38 PM.png - 103kB](https://www.sciencemadness.org/whisper/files.php?pid=242297&aid=18055)
Vikascoder - 23-3-2012 at 01:40
Watch the chemlife video on youtube how to make potassium perchlorate from matches . According to him you have to use non safety matches but safety
matches work to . Another way is in place of matches use potassium chlorate in place of matches and dont add ammonia . Another method you can try to
do electrolysis of potassium chloride with lead dioxide anode
woelen - 23-3-2012 at 02:21
There are several ways of making KClO4, none of them being particularly easy if you don't have the right equipment. As Fleaker suggested, please use
the search engine and do some more research instead of asking to be spoonfed.
As a starter, in google type: potassium perchlorate site:*.sciencemadness.org
This thread is closed now.