Wheaton 400, also known as No-Sol-Vit, is a borosilicate glass that falls well within the limits for USP Type I chemically resistant borosilicate
glass, as specified in the XXIII revision of the U.S. Pharmacopoeia. Examples include safety-coated wide-mouth bottles 34501-20, -50 and -70.
|