500 gms of CELITE diatomaceous earth was mixed with 1320 gms of liquid ammonium phosphate fertilizer. The fertilizer contained 34% P2O5. The
semi-solid resulting from the mixture was dried at 105C. and milled to 14 meshparticles. The P2O5 content of the dry solid was found to be 36%.
|