Any one has information about Aluminum ethoxide?ScienceSquirrel - 8-6-2011 at 06:49
Melting point 140 C
Moisture sensitive
Prepared in the same way as aluminium isopropoxide, reflux aluminium in the alcohol in the presence of mercury chloride as a catalyst.Waffles SS - 8-6-2011 at 07:18