Quote: Originally posted by Delta-R ![](images/xpblue/lastpost.gif) | Agreed - the samples that were left for the whole distillation were very highly nitrated - they do not dissolve in acetone, just leaving a clumpy,
fibrous mass, and they VIOLENTLY ignite and disappear with no ash whatsoever. |
Doesn't highly nitrated cellulose dissolve in acetone? |