can someone help me to solve chemical reaction
fecl3(liquid) + cu(solid)=???
Mr joey
-
1-3-2011 at 02:39
how to make electrolysis to get copper?
hissingnoise
-
1-3-2011 at 06:55
Quote:
how to make electrolysis to get copper?
The question is vague, but anyway . . .
Impure copper is purified by electrolysis by making it the anode and plating it onto a cathode of pure copper.
And; FeCl<sub>3</sub> + Cu --->FeCl<sub>2</sub> +CuCl
The reaction barely proceeds in the absence of O<sub>2</sub>.