Quote: Originally posted by Brightthermite ![](images/xpblue/lastpost.gif) |
Freeze precipitation it what I found to work best after a lot of struggling. I would boil the solution down to much and the second it came in to
contact with anything that was of a slightly cooler temp, the AN immediately caked on in a hot sludge.
Please keep me updated on the drying, I am having a very hard time oven drying and keep moister out if it in general (around 80% humidity constantly).
|
The AN was split into two batches and spread in a glass baking pan. The pan was heated to 70-90 C (kind of varied) in a conventional oven, the door
propped slightly open with a spoon to promote airflow. Every 30-60 minutes AN was stirred/scraped. Total drying time was about 10 hours, to constant
mass. All AN was passed through a kitchen sieve and the remaining pieces were ground with a mortar and pestle until they would pass through a sieve.
Total mass was about 3.5 pounds of free flowing, snow white AN which was stored in an ordinary ziploc. I guess the filtrate should have been boiled
down a bit more, oh well.
https://i.imgur.com/G8FMXrf.jpg
Mortar and pestle definitely sucks but I don't have the balls to use a coffee grinder or a food processor. Maybe with a 100 foot extension cord. |