Ubya - 30-4-2020 at 08:10
for my graduation my friends bought me a 50cm glass gravity chromatography column, it looks huge. I've never used it yet as i'm still making the
silica gel powder for it. since i broke an addition funnel while trying to repair it, i check all my glassware for internal stress, i just look at the
piece of glassware between a polarizing filter and my laptop screen showing a white background. checking this column i noticed some pretty evident
stress rings
![20200430_175413-1.jpg - 2.2MB](https://www.sciencemadness.org/whisper/files.php?pid=635084&aid=80769)
i would hate to break it while using it, so i'd like to anneal it somehow.
any ideas on how in a home envirorment?
Deathunter88 - 1-5-2020 at 01:38
You're only going to make it worse. Chromatography columns aren't heated so it will be fine.
Ubya - 1-5-2020 at 09:34
i hope that if i ever apply some positive pressure to speed the flow it doesn't crack or break