By evaporating it down in the open bowl all the ammonia hydroxide will evaporate out as well. That's what makes the disgusting smell, ammonia. Much
easier to freeze urine, water will freeze up, but all the compounds that decomposes to ammonia hydroxide will stay liquid. Pour out water. Then just
distill off almost pure ammonia hydroxide solution, you need to watch it because when it gets to hot, it foams and can contaminate colourless
distillate. I used to etch PCBs with it, had litres of copper ammonium complex. And you don't need to add anything to it!
[Edited on 4-4-2020 by Romix] |