Lion850 - 13-2-2020 at 20:08
Hi Aussie members,
Looks this eBay seller from Melbourne has added a few items at what appears to be reasonable pricing:
https://www.ebay.com.au/sch/victoria-hardware/m.html?_nkw=&a...
I've ordered the cerium oxide.
Kobold vor NH4 - 14-2-2020 at 01:50
Interesting, I'll probably get some CeO2 as well, maybe some NaBr.
I also found this place while I was look around for pottery supply stores.
/
https://www.potterysuppliesonline.com.au/Products.html
Look in the >Powdered Oxides< and the >Raw Materials-Powder< categories.
I haven't yet ordered from yet but I plan to. They don't accept online payments, just bank transfer and credit card, however I plan on buying in
person next time I'ma in Brisbane.
B(a)P - 14-2-2020 at 02:06
Thanks for the heads up, some interesting items in there. Unfortunately just today I purchased some sodium nitrite for more than what they are asking.
It was AR though.