Is stainless steel resistant to copper sulfate and strong acids?
fusso - 20-4-2019 at 06:12
No, it will dissolve in HCl.
Bedlasky - 20-4-2019 at 06:17
Thank you.
Felab - 20-4-2019 at 08:13
It depends on which type of stainless steel. 316 stainless steel will resist HCl for example.