Pumukli - 28-1-2019 at 10:13
I've found this interesting thermit demonstration experiment and uploaded it here for your entertainment. ![:)](./images/smilies/smile.gif)
(I was searching "aluminum foil activation" on the net while came across this gem.)
Just read it and try - if you have the balls. ![:D](./images/smilies/biggrin.gif)
And please report back!
Attachment: rustyballthermite.pdf (155kB)
This file has been downloaded 433 times
[Edited on 28-1-2019 by Pumukli]
DraconicAcid - 28-1-2019 at 21:16
I do that all the time for my students. I went to the metal scrap people and asked them if they had any tekk bearings- they are just the right size.
wg48 - 29-1-2019 at 01:37
I once found some reels of old magnetic tape. I assumed it was coated with a magnetic oxide perhaps an iron oxide. Using pieces of the tape and
aluminium foil I made a thick sandwich of alternative sheets of the tape and foil. I then heated the sandwich slowly hoping to volatilise the plastic
of the tape and leave a thermite mixture that would ignite when it was hot enough. It never did ignite but while it was being heated strongly it made
a succession of pops and crackes which I assumed were small areas of aluminium and oxide that reacted explosively.
I guess the pops and cracks could also have been the sudden release of trapped gases from the decomposition of the plastic.
FeedMe94 - 29-1-2019 at 01:56
Awesome idea , i will give it a try. A friend of mine have some old rusty cannon balls , solid iron
Ubya - 29-1-2019 at 02:54
myst32YT showed it 9 years ago. https://www.youtube.com/watch?v=rqXP-yUT_zI
FeedMe94 - 29-1-2019 at 08:35
A bit off topic but i will give it a go if you dont mind
Here where i live , the older guys , every easter make a white paste and use to cover big round pebbles from the beach. Then they throw it to a
downslope and the pebble exploding everytime it hits the road. Any idea what this is ?