Go to a plumbing specialist supplier and get them to order in 1" wide gas sealing teflon tape. This is high density TFPE, by standard, not the low
density PTFE used for water pipe. The extra width means you need few overlaps and hence this lessens the stress issues inherent with using tape. I
have not assessed this conclusion just supposed it.
|