Search |
[Next Page] |
The Short Questions Thread (4) Hmm... then I might get a glass stem tube thermometer adapter then, just to be safe.
I'm asking b ... |
17-12-2017 at 18:40 by: ninhydric1 |
The Short Questions Thread (4) Would this thermometer adapter:
https://www.ebay.com/itm/Glass-Thermometer-Adapter-With-Thread-24 ... |
17-12-2017 at 17:24 by: ninhydric1 |
Looking for Textbook Answers This is what you might be looking for, but it is quite pricey:
https://www.walmart.com/ip/Organic-C ... |
15-12-2017 at 22:07 by: ninhydric1 |
What on earth is my "Pyridine"?! Try boiling point and freezing point first. These are usually good for indicating organic compounds ... |
10-12-2017 at 11:55 by: ninhydric1 |
Addition of HCl to Propenoic acid I would assume LearnedAmateur's mechanism is correct, as only HBr can undergo free-radical addition, ... |
9-12-2017 at 14:43 by: ninhydric1 |
What were your first experiments when you got in to this hobby? My first experiment was the distillation of denatured ethanol (No, I was not trying to make potable ... |
27-11-2017 at 17:36 by: ninhydric1 |
newly-discovered, naturally-occurring photonuclear reaction If you want I can send you the whole article. U2U me for access. |
26-11-2017 at 15:35 by: ninhydric1 |
Preparation of titanium nanoparticles I assume plante1999 meant that the reaction takes place when Na2S2O7 starts melting. I'm pretty sure ... |
25-11-2017 at 13:26 by: ninhydric1 |
Preparation of titanium nanoparticles TiO2 is often used in photocatalyzing specific reactions so it would make sense that it is an experi ... |
25-11-2017 at 09:43 by: ninhydric1 |
Is it possible to fuse carbon fiber and diamonds to form a harder material? You can indeed make graphene from graphite, which indeed is a surprisingly strong material with nume ... |
24-11-2017 at 22:40 by: ninhydric1 |
Preparation of Oleum by Use of Phosphoric Acid For the prep of thionyl chloride I assume? Can't wait for that! |
24-11-2017 at 19:41 by: ninhydric1 |
Preparation of Quinoline Beautiful write-up as usual Magpie; always admired your work. By the way, what do you plan to do wit ... |
23-11-2017 at 19:07 by: ninhydric1 |
Dense, metallic liquid - supposed mercury - hit or shit? If you want to clean it chemically, some HCl or dilute H2SO4 will be good enough. The pinhole is the ... |
23-11-2017 at 12:46 by: ninhydric1 |
Dense, metallic liquid - supposed mercury - hit or shit? It will dissolve in hot concentrated sulfuric acid. |
23-11-2017 at 10:53 by: ninhydric1 |
The lead salts preparation thread! Are lead fishing sinkers pure lead or is the lead sometimes contaminated with antimony and/or other ... |
23-11-2017 at 10:44 by: ninhydric1 |
Preparation of titanium nanoparticles I have recently taken an interest in nanoparticles and their versatile applications and developments ... |
22-11-2017 at 21:34 by: ninhydric1 |
Fresh, minty smell from addition of Cu(OH)2 to con. NaOH soln. Or maybe you were making some methyl salicylate around the same time you were performing this reacti ... |
21-11-2017 at 21:50 by: ninhydric1 |
The Short Questions Thread (4) Would a paint can hold up against plante1999's synthesis of TiCl4, as quoted below (assuming it actu ... |
21-11-2017 at 21:47 by: ninhydric1 |
Hard balancing You could probably apply Cramer's Rule to these matrices but finding the determinants for 5x5 matric ... |
19-11-2017 at 19:31 by: ninhydric1 |
Diclhloromethane synthesis Here it is @dan_vlad. |
19-11-2017 at 10:09 by: ninhydric1 |
How to make chromium (III) oxide (Cr2O3) The OP says that he wants to make potassium dichromate, so wouldn't alkali hydroxides be OK for the ... |
16-11-2017 at 07:36 by: ninhydric1 |
Transition (and other) metal salts of Carboxylic Acids and their properties The manganese salts have the characteristic pale pink color of manganese in the 2+ oxidation state s ... |
15-11-2017 at 20:45 by: ninhydric1 |
Sulforaphane Ethanol should work but it may dissolve much more unwanted material from the broccoli, while nitrile ... |
15-11-2017 at 20:35 by: ninhydric1 |
How to make chromium (III) oxide (Cr2O3) If nitric acid is cheap for you (definitely not for me), allow the metal to sit in the acid until no ... |
15-11-2017 at 20:33 by: ninhydric1 |
Isolation of elemental Boron and Proof Demonstrations of Allotropes You did poke it with a graphite rod. Maybe pieces of the rod broke off without you knowing? |
13-11-2017 at 18:50 by: ninhydric1 |
[Next Page] |