Unified Copper Process
Well, I've already got it to where I can generate H2S on demand. The reactions of chlorine and H2S ...
29-6-2008 at 16:21
by: kilowatt
Unified Copper Process
After some experimenting I am leaning towards a calcium sulfide route to the SO2 for this process fr ...
28-6-2008 at 18:45
by: kilowatt
Condensing chlorine gas, price of ethane!!!!
I think once you sell them, you will later find that you really did need them, and regret selling th ...
18-6-2008 at 19:43
by: kilowatt
Condensing chlorine gas, price of ethane!!!!
If it goes to -85°C then you can use it to make dry ice by condensing CO2 from a tank or even as it ...
18-6-2008 at 15:50
by: kilowatt
Recasting teflon
There is a fine line between melting and decomposition (to deadly gases such as HF and fluorophosgen ...
13-6-2008 at 15:16
by: kilowatt
Glass or teflon stop cock?
[quote]
I don't have access to a torch, so I cant really heat just the outside joint.[/quote]
Just ...
13-6-2008 at 08:59
by: kilowatt
Glass or teflon stop cock?
Teflon stopcocks shrink and expand greatly with temperature, and as such can easily come loose if th ...
12-6-2008 at 20:21
by: kilowatt
Easy production of ammonia?
[quote]
haha... funny story, i don't know of any ammonium products that I can get my hands on... or ...
31-5-2008 at 01:21
by: kilowatt
Sword Forging!
Did you pay extra for the premium sword quenched in elf blood or something? No mortal sword can cut ...
17-5-2008 at 14:35
by: kilowatt
Sword Forging!
He is being sarcastic. A good sword would just bounce off all those items (and chip the edge) if it ...
17-5-2008 at 11:04
by: kilowatt
Barium Metal
I would just coat it in thick wax and cut it with a hand saw of whatever type. If the shavings are ...
16-5-2008 at 09:43
by: kilowatt
Sword Forging!
[quote]
All of them are steel alloys, and no other metals can compare[/quote]
There are some nicke ...
15-5-2008 at 05:20
by: kilowatt
Unified Copper Process
Does CaB4O7 have any uses that might interest me?
14-5-2008 at 17:05
by: kilowatt
Unified Copper Process
[quote]
I'm not sure if Ca2SiO4 exists and what its properties are. [/quote]
Ca2SiO4 is calcium or ...
14-5-2008 at 15:23
by: kilowatt
Unified Copper Process
I have begun to experiment with the reaction of calcium sulfate with carbon and silica at high tempe ...
14-5-2008 at 10:13
by: kilowatt
PVD at home
[quote]
Is terra cotta a suitable refractory material or am I living in dreamland?[/quote]
Maybe; ...
13-5-2008 at 21:25
by: kilowatt
Separation of Copper/Nickel Alloy
[quote]
Copper sulfate decomposes to the oxide at about 650 C, nickel sulfate at about 850 C. If th ...
19-4-2008 at 13:15
by: kilowatt
worst stench
I have a friend that works at the local apiary, and would often come home smelling like butyric acid ...
18-4-2008 at 15:23
by: kilowatt
Separation of Copper/Nickel Alloy
[quote]
Otherwise, isn't one of 'em magnetic?[/quote]
Only in metallic form, below its austenitic ...
18-4-2008 at 09:30
by: kilowatt
Separation of Copper/Nickel Alloy
[quote]
It would seem an easy task to dissolve the metals as a sulfate with an electrolytic cell, u ...
17-4-2008 at 22:47
by: kilowatt
Unified Copper Process
Copper(I) chloride precipitates out when copper(II) chloride reduced by sulfite, but I am aware that ...
17-4-2008 at 22:12
by: kilowatt
Unified Copper Process
I know of nowhere where I can buy sulfur for anywhere near the price of gypsum (I can get scrap dryw ...
17-4-2008 at 21:47
by: kilowatt
Separation of Copper/Nickel Alloy
It would be pretty hard to leech all the copper out with ammonia I think, much as it would be pretty ...
17-4-2008 at 21:16
by: kilowatt
Separation of Copper/Nickel Alloy
That copper (II) aspirinate looks really promising, fast and easy, and high yield as long as nickel ...
17-4-2008 at 20:26
by: kilowatt
Unified Copper Process
I may have come up with a relatively straightforward process that unites the production of sodium hy ...
17-4-2008 at 19:27
by: kilowatt
[Next Page]

  Go To Top