Search |
[Next Page] |
Thoughts On Anodes Aren't you planning to use some sort of interface coating on the substrate before you plate on the P ... |
23-12-2008 at 15:18 by: Rosco Bodine |
Thoughts On Anodes It's a conductor, but an ionic barrier to oxygen, I'm pretty sure. That is what made me think you w ... |
23-12-2008 at 15:07 by: Rosco Bodine |
Thoughts On Anodes If you are talking again about cerium, I really think that angle is something which would have to be ... |
23-12-2008 at 10:26 by: Rosco Bodine |
Thoughts On Anodes [quote][i]Originally posted by Swede[/i]
Roscoe, I am interested in all forms of this process, and ... |
22-12-2008 at 18:27 by: Rosco Bodine |
Thoughts On Anodes I'll go out on a limb here and suggest something untried and unreported which might make an interes ... |
21-12-2008 at 20:59 by: Rosco Bodine |
Thoughts On Anodes The type of alumina we were curious may have value is a nano structural whisker, a fiber form of mat ... |
18-12-2008 at 20:47 by: Rosco Bodine |
PETN synth An educated guess is that your problem is related to two factors...reaction temperature too low and ... |
17-12-2008 at 02:14 by: Rosco Bodine |
The short questions thread (1) Nitroethane could possibly be reduced to ethylamine.
Al amalgam or Al isopropoxide would probably d ... |
17-12-2008 at 01:05 by: Rosco Bodine |
PETN synth Yeah I have studied this nitration a bit and worked out
a pretty optimal synthesis which is basical ... |
15-12-2008 at 18:18 by: Rosco Bodine |
Thoughts On Anodes Kaowool and a blender maybe
I would try the long fiber stuff and low porosity, specify
a fill ... |
12-12-2008 at 17:08 by: Rosco Bodine |
Thoughts On Anodes Please indulge my off topic diva break, this is too beautiful to go unlinked and worth the listen
... |
11-12-2008 at 20:10 by: Rosco Bodine |
Mr. Anonymous: HgCl2 prep Hmmm, maybe Mr. A is onto something there |
11-12-2008 at 01:05 by: Rosco Bodine |
another organic precursor MMO of possible interest The last part of page 172 and all of page 173 in this book preview shows use of citric acid and ethy ... |
10-12-2008 at 20:29 by: Rosco Bodine |
Thoughts On Anodes You can't dehydrate nickel nitrate by heating without decomposing it to a basic nitrate and then to ... |
10-12-2008 at 16:26 by: Rosco Bodine |
Niobium pentoxide wanted Actually niobium doping of titanium oxide and also
possibly spinels containing a niobium oxide comp ... |
10-12-2008 at 02:03 by: Rosco Bodine |
Thoughts On Anodes Actually the watts drops to 25% at half voltage because the amperage also halves ....I favor incoloy ... |
5-12-2008 at 17:59 by: Rosco Bodine |
Thoughts On Anodes Omega ..Oh man ...grab your wallet before they do ....
sheesh
On those cartridge heaters, if ... |
5-12-2008 at 14:10 by: Rosco Bodine |
Thoughts On Anodes Here is another possible supplier
http://www.wesbond.com/colloidal_alumina.htm
and another
http:/ ... |
30-11-2008 at 08:09 by: Rosco Bodine |
commercial availability The fibrous alumina is commercially available since it is used as thickener for lubricants, cosmetic ... |
29-11-2008 at 08:54 by: Rosco Bodine |
Amalgamated Aluminum at ordinary conditions Cobalt doping of the gamma alumina resulting after pyrolysis will result in cobalt aluminate spinel ... |
28-11-2008 at 18:55 by: Rosco Bodine |
US3039849 Amalgam Derived Fibrous Alumina I don't see that one sorry. It seems like a more complex route than working with the precursor which ... |
28-11-2008 at 11:32 by: Rosco Bodine |
Thoughts On Anodes Yeah the nanostructured alumina whiskers are sort of an ultimate form of "activated" alumina, having ... |
28-11-2008 at 10:59 by: Rosco Bodine |
Thoughts On Anodes Yeah I saw that reference along the way to requesting the book. Evidently it is the highly activate ... |
28-11-2008 at 10:28 by: Rosco Bodine |
Thoughts On Anodes A couple of references have turned up saying that fibrous alumina is the form of the oxide which gro ... |
28-11-2008 at 08:54 by: Rosco Bodine |
Thoughts On Anodes Really though what I said about the Pytlewski polymer is important and it contains the bismuth dopan ... |
26-11-2008 at 15:00 by: Rosco Bodine |