Help me deplate something IRC the book even mentions that the sulfide films are delicate. I would think several layers of sp ... |
20-6-2009 at 06:37 by: chloric1 |
Help me deplate something What really turns me on is the book writen by the owner of Sculpt Nouveau. I like the fuming method ... |
19-6-2009 at 18:55 by: chloric1 |
Help me deplate something Yes watson, I have a couple patina books. This is where I drew my ideas from. I paid out $85 for m ... |
19-6-2009 at 17:49 by: chloric1 |
Help me deplate something Certain metal salt solutions are causitc and discolor metal surfaces. I know Antimony chloride is f ... |
19-6-2009 at 16:39 by: chloric1 |
Iodomethane prep. I remember one time going into the liquor store buying a fifth of everclear and taking it home and n ... |
19-6-2009 at 15:10 by: chloric1 |
Best and worst smelling chemicals? Jor you are right. I feel comfortable working with halogens, SO2,NO2,and HCl outside. Hydrogen sul ... |
9-6-2009 at 15:44 by: chloric1 |
Best and worst smelling chemicals? I have thought about the fume hood. But I am limited on storage space and I do virtually all chemis ... |
8-6-2009 at 18:18 by: chloric1 |
Best and worst smelling chemicals? Bromine! I love the chemistry but I HATE the smell and the effects! Chlorine is "sharper"if that m ... |
8-6-2009 at 16:18 by: chloric1 |
HCl Preparation with no other strong acid
[quote]
You can add the chlorine to water to make hypochlorous acid (HClO). Let that stand long e ... |
8-6-2009 at 08:28 by: chloric1 |
Ferricyanide precipitation? Yes some labware is expensive but stoppers are not. You can buy huge bags of stoppers on ebay. If ... |
1-6-2009 at 16:17 by: chloric1 |
Cr2O3 can be dissolved in water easily [rquote=151188&tid=12099&author=kclo4][quote]Also, it is a good color for cold process soap! ... |
15-4-2009 at 07:00 by: chloric1 |
Zinc in brass does not react with acids? Brass is definately not the idea source for zinc. Copper sulfate is actually a catalyst to assist i ... |
14-4-2009 at 16:04 by: chloric1 |
Cr2O3 can be dissolved in water easily Damn! I sold all my Cr2O3 on ebay![:(](./images/smilies/sad.gif) !!
I will have to get more when I order V2O5 or Fe3O4. In ... |
14-4-2009 at 15:55 by: chloric1 |
Something Else to Do with Your Red P A vapor phase reaction might be in order here. Just heat PCl5 in a flask to vaporization and drive ... |
15-2-2009 at 07:20 by: chloric1 |
Preparation of dilute hydrazine from N2H4.2HCl Woelin sounds like you got a interesting method here I would love to know the outcome.
[quote]
A ... |
8-2-2009 at 07:53 by: chloric1 |
Thoughts On Anodes [quote]
The price at $10/sheet is cheaper per square inch than the stuff I bought earlier... might ... |
7-2-2009 at 17:33 by: chloric1 |
Underground Gadgets & Chemical Supply Panzi, you are absolutely right, but why ask why? As long as something is a good deal and if the pr ... |
4-2-2009 at 13:25 by: chloric1 |
Underground Gadgets & Chemical Supply Who wants 19 liters of HCl for 125 BUCKS! Are you kidding me?! I don't know about you but selling ... |
31-1-2009 at 11:51 by: chloric1 |
Blowing up a resistor at the end of 100m of wire What a cool thread! I will definately look into 'exploding wires" soon. I heard of this 10 years a ... |
30-1-2009 at 11:30 by: chloric1 |
Underground Gadgets & Chemical Supply [quote][i]Originally posted by hissingnoise[/i]
[quote][i]Originally posted by chloric1[/i]
Also, ... |
29-1-2009 at 15:25 by: chloric1 |
Underground Gadgets & Chemical Supply Yes that would be the right path to go. Small labs and educational institutions usually have more c ... |
29-1-2009 at 09:03 by: chloric1 |
Underground Gadgets & Chemical Supply Well cracker, you where very professional and considerate with me in the email you sent. I was the ... |
28-1-2009 at 19:15 by: chloric1 |
Intelligent Acquisition of Reagents [quote]
Well, seems like the developing countries might offer a little more freedom for what you're ... |
19-1-2009 at 07:45 by: chloric1 |
Why you should always dispose properly of your chemical waste Its real but vulture is right, they atually have to tap into your connection.
But, in the event ... |
13-1-2009 at 17:37 by: chloric1 |
periodic acid synthesis [quote][i]Originally posted by not_important[/i]
SrSO4 Solubility in water 0.0135 g/100 ml (25°C ... |
12-1-2009 at 08:22 by: chloric1 |