Carbon Foam Refractory Made From Bread
I am glad I dug up that original item about making carbon refractory with kitchen chemistry! It look ...
19-11-2016 at 15:54
by: careysub
Briggs–Rauscher reaction - Chemical Oscillations
The original observation of oscillating chemical reactions by Belousov was in a system that had citr ...
18-11-2016 at 08:22
by: careysub
Red chemiluminescence
Woelen recommends also doing the singlet oxygen demonstration with sodium dichloroisocyanurate, prov ...
17-11-2016 at 14:26
by: careysub
Help Buying Platinum Leaf
I follow this philosophy with some other metals in my collection - if it is relatively expensive, I ...
16-11-2016 at 07:42
by: careysub
Help Buying Platinum Leaf
[rquote=466745&tid=70847&author=Chemetix]I have samples of each of the metals in the form of ...
15-11-2016 at 12:03
by: careysub
Help Buying Platinum Leaf
[rquote=466740&tid=70847&author=Maroboduus][rquote=466736&tid=70847&author=careysub] ...
15-11-2016 at 12:00
by: careysub
Help Buying Platinum Leaf
Not claiming that leaf is cheaper from the UK on a per-leaf basis, it is just if I want a couple I d ...
15-11-2016 at 09:10
by: careysub
Help Buying Platinum Leaf
[rquote=466714&tid=70847&author=Maroboduus]@carreysub: Have you dealt with gold leaf before? ...
14-11-2016 at 20:24
by: careysub
Help Buying Platinum Leaf
Hmm... I haven't called up the Australian supplier yet, I'll keep trying, but I found a U.S. supplie ...
14-11-2016 at 17:50
by: careysub
Help Buying Platinum Leaf
I would like to acquire platinum, 24 K gold, and palladium leaf for my element collection. Gilding a ...
14-11-2016 at 17:22
by: careysub
Nanotech article series (some of my work, a review and future outlooks of the field)
Between this and the carbon foam thread, we have the materials of the future being made in kitchens ...
11-11-2016 at 15:59
by: careysub
Nitric Acid from Calcium Nitrate
Just a thought - would it work to make copper nitrate from calcium nitrate using metathesis with cop ...
10-11-2016 at 13:06
by: careysub
PVC ducting
PVC is rated for use with sulfuric acid of any concentration less than "fuming" at room temperature, ...
7-11-2016 at 07:39
by: careysub
Carbon Foam Refractory Made From Bread
[rquote=466022&tid=70570&author=Maroboduus]Morgan's thoughts on pore size make a lot of sens ...
4-11-2016 at 12:48
by: careysub
Carbonate test for neutrons
Since nuclear transformations involve a million times as much energy as a chemical transformation (a ...
4-11-2016 at 10:58
by: careysub
Refractory with flour or saw dust incorporated?
If you want something with significant insulating value try using perlite or coarse vermiculite with ...
3-11-2016 at 15:32
by: careysub
Long term experiment: does this make chlorosulfonic acid?
Maybe this will some day go into the annals with the Pitch Drop Experiment:

https://en.wikipedia. ...
3-11-2016 at 11:46
by: careysub
Benzaldehyde on Amazon Prime?
[rquote=465866&tid=70340&author=Camroc37]

I noticed that a lot of people on eBay were sel ...
2-11-2016 at 19:32
by: careysub
Benzaldehyde on Amazon Prime?
[rquote=465833&tid=70340&author=Maroboduus][rquote=465822&tid=70340&author=Khemi]Is ...
2-11-2016 at 15:24
by: careysub
Carbon Foam Refractory Made From Bread
[rquote=465838&tid=70570&author=j_sum1]It is notable that the shape of the material distorts ...
2-11-2016 at 15:03
by: careysub
Carbon Foam Refractory Made From Bread
My particular interest is its usability as a high temperature insulator.

Above 1650 C there aren ...
2-11-2016 at 13:41
by: careysub
Benzaldehyde on Amazon Prime?
Note that "bitter almond essential oil" is basically just benzaldehyde. And it is widely sold.

Ch ...
2-11-2016 at 12:53
by: careysub
Carbon Foam Refractory Made From Bread
I agree with Aga, this topic is good one for further amateur work at extending it.
2-11-2016 at 12:36
by: careysub
Carbon Foam Refractory Made From Bread
[rquote=465811&tid=70570&author=MrHomeScientist]I'm sure the density difference is why wood ...
2-11-2016 at 11:59
by: careysub
Carbon Foam Refractory Made From Bread
I will bet that both nitrogen and carbon dioxide will work pretty well. After all carbon is pretty i ...
1-11-2016 at 18:11
by: careysub