Etching or anodizing tin For a art project I have to etch tin. I tried a few things I tired anodizing it with 3,6,12v with so ... |
26-2-2018 at 04:54 by: Foeskes |
Can butane melt silver? [rquote=503196&tid=79519&author=zed]Now, if you have an old microwave oven or two, and a lan ... |
9-1-2018 at 14:51 by: Foeskes |
Can butane melt silver? Just tried melting a small amount of it it melted no problem. |
6-1-2018 at 17:15 by: Foeskes |
Sodium and CuSO4*5H2O Impact sensitive i tried putting a small amount of sodium(around 1mm^3)on a 'anvil'(just a large sledge hammer), then ... |
6-1-2018 at 01:44 by: Foeskes |
Can butane melt silver? I extracted some silver from a bracelet I bought. Not its a gray powder. After converting to silver ... |
5-1-2018 at 21:43 by: Foeskes |
Storing nitrogen in ampoule I'm going to store nitrogen in a ampoule. But I'm not completely sure if I way I'm going to make it ... |
24-12-2017 at 18:06 by: Foeskes |
Failed chrome alum synthesis The longest side is 6mm
Edit: after leaving for 24 hours there are 3 large crystals, unfortunately ... |
8-12-2017 at 16:08 by: Foeskes |
Failed chrome alum synthesis Here is my attempt:
I used K2Cr2O7(10g) and I dissolve it in 50ml of water.
In an ice bath I added ... |
7-12-2017 at 23:00 by: Foeskes |
What to do with aluminum shavings? I found I video by a Russian guy named "dr nitro crazy scientist" or something like that he used alu ... |
2-12-2017 at 01:53 by: Foeskes |
Isolation of elemental Boron and Proof Demonstrations of Allotropes I like to heat Boric acid on steel cans because after it freezes you can smash the bottom of the can ... |
21-11-2017 at 20:55 by: Foeskes |
Trouble with getting nickel(II) to dissolve in ammonia. It's 25% |
12-11-2017 at 20:59 by: Foeskes |
Trouble with getting nickel(II) to dissolve in ammonia. I don't really have any concentrated acetic acid, only vinegar. |
12-11-2017 at 19:05 by: Foeskes |
Trouble with getting nickel(II) to dissolve in ammonia. I am trying to separate nickel from iron and chromium. I first dissolve the metal in HCl and precipi ... |
12-11-2017 at 18:12 by: Foeskes |
Melting fine bismuth powder I managed to melt it into small nuggets!
After trying the wax thing which failed, I decided to mix ... |
25-10-2017 at 17:04 by: Foeskes |
Are metal ammine complexes unstable in concentated sodium hydroxide solution? I'm going to precipitate separate nickel and chromium from iron by complexity them with ammonia and ... |
13-10-2017 at 21:50 by: Foeskes |
Will nickel(II) hydroxide react with sodium hypochlorite or hydroxide? So is sodium hydroxide the most ideal for dissolving the chromium and leaving the nickel behind?
Ac ... |
12-10-2017 at 16:50 by: Foeskes |
Will nickel(II) hydroxide react with sodium hypochlorite or hydroxide? Doesn't Sodium hydroxide react to form chromite?
And what about hypochlorite? |
11-10-2017 at 14:29 by: Foeskes |
Will nickel(II) hydroxide react with sodium hypochlorite or hydroxide? I am going to try to separate nickel from chromium.
I'm thinking of using either reacting their hyd ... |
11-10-2017 at 05:25 by: Foeskes |
Bismuth powder melting Try adding paraffin wax(a little bit of it) and the close the crucible redirect the vent hole of the ... |
11-10-2017 at 05:12 by: Foeskes |
The Slime craze!! [rquote=493931&tid=77309&author=NEMO-Chemistry]I got no where using PVA glue sold in the Uk ... |
7-10-2017 at 15:59 by: Foeskes |
'Invisible sodium' effect using nitric acid Today I accidentally made 'invisible sodium' similar to thoisoi2's video, but using dilute 2M nitric ... |
6-10-2017 at 22:42 by: Foeskes |
Making ferrate(Fe VI+) I tried the volcano method, but it seems like unless you have extremely fine iron powder(like fine b ... |
6-10-2017 at 01:15 by: Foeskes |
Chromium from thermite When breaking the slag the were small beads of chromium and after breaking one, it was pretty shiny. ... |
22-9-2017 at 18:54 by: Foeskes |
Chromium from thermite I recently made chromium from thermite.
The recipe I used was 20 grams Cr2O3:12 grams K2Cr2O7:11.4 ... |
22-9-2017 at 17:51 by: Foeskes |
What are "synthetic iron oxides" I might buy some later and post a image. Maybe it's Prussian blue? Since it's name is pretty mislead ... |
22-9-2017 at 17:44 by: Foeskes |
[Next Page] |