Why does my Mg-Cu galvanic cell produce the wrong voltage? The table you are looking at is for 'standard' conditions.
The concentration partially determines w ... |
30-11-2023 at 09:14 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Experiment #492, start.
7 drops acetic acid, 21 drops ester with multiple oxygen count, sea-salt (N ... |
29-11-2023 at 15:52 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Last night, when I saw the carmel color in the choline, I suspected the tube was going to go totally ... |
29-11-2023 at 10:30 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Expriment #491
Choline chloride: 136 [g/mol]
Urea 60.0 [g/mol]
Eutectic is 1:2 molar mixture. ... |
28-11-2023 at 14:51 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. I have choline chloride; I have urea, and I have thiourea.
I also have propylene-diol, and n-propan ... |
28-11-2023 at 13:25 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. While I wait for a more specific suggestion ... I tried an ester + carboxylic acid, spiked with a ti ... |
28-11-2023 at 09:44 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. I found this, which is a little more detailed than the wikipedia article.
[url=https://chem.libre ... |
27-11-2023 at 11:47 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Hi, thanks for the suggestion.
I do have propylene carbonate reagent grade, (Southern tier scient ... |
26-11-2023 at 20:40 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. I'm happy to read old sources from online. I can even run a few experiments in water. But, I don't ... |
26-11-2023 at 10:30 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Bubbling has accelerated, current remains at 1[mA]. Experiment #490, the "ether" variation.
Notice ... |
24-11-2023 at 11:05 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. [quote]If I had the time to mess around with nickel processes, I would be focusing on REMOVING nicke ... |
24-11-2023 at 09:15 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Note: From my transfer pipette, I counted the drops from the 1/2cc mark; and 24 drops of ether is 1/ ... |
23-11-2023 at 19:53 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. [rquote=688850&tid=159974&author=Rainwater]This suggestion is expensive and dangerous, reall ... |
23-11-2023 at 19:41 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Um, if you mean my persistence, then I agree; but I really only have an undergraduate course in inor ... |
23-11-2023 at 15:53 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Unusually nice.
This morning, all solds were dissolved. Centerfuging, not needed.
From the di ... |
23-11-2023 at 08:41 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Today's experiment, #490
I've got some plating activity on the higher current electrode.
Not sur ... |
22-11-2023 at 22:49 by: semiconductive |
Using Corning PC-425D on 240V After looking at the pictures, I'm going to say the answer is NO. You will have trouble using this ... |
22-11-2023 at 14:17 by: semiconductive |
Using Corning PC-425D on 240V [rquote=688793&tid=159982&author=print118]I made an error with the model, my apologies. The ... |
22-11-2023 at 13:59 by: semiconductive |
Laboratory power supply constant current How constant of a current do you want?
A light bulb filament happens to be a decent current regul ... |
21-11-2023 at 23:36 by: semiconductive |
What happens to capacities of batteries when connected in series or parallel? [rquote=373209&tid=44458&author=unionised][rquote=363242&tid=44458&author=franklyn]S ... |
21-11-2023 at 23:26 by: semiconductive |
Using Corning PC-425D on 240V I don't have one to check.
But: I know that the 240V corning plate and 120V corning plate have th ... |
21-11-2023 at 23:03 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. All comments, welcome; Thanks!
Anode material, pure nickel wire, 0.9mm diameter, spooled around 6 ... |
21-11-2023 at 18:32 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. I've been experimenting for around two years with electroplating of metals in orgainc liquids. I've ... |
19-11-2023 at 15:09 by: semiconductive |
Questions in electroplating I'm less knowledgeable than others here; I've been experimenting with waterless plating of iron for ... |
19-11-2023 at 14:32 by: semiconductive |
methanol/ionic liquid electroplaing of metals [rquote=659572&tid=157386&author=clearly_not_atara]pKa H2O: 15.7