Search |
[Next Page] |
OTC tert-Butanol [rquote=258395&tid=21341&author=elementcollector1]Is there any way to turn MTBE into T-butan ... |
1-9-2012 at 02:03 by: Dave Angel |
Sodium! Thanks for the words of encouragement [b]Tank[/b]! This is one of the more involved projects I've ta ... |
27-8-2012 at 09:59 by: Dave Angel |
Thorium Separation From TIG Electrodes [rquote=257563&tid=11275&author=vmelkon]The packaging should say 2% thoriated. The rods are ... |
21-8-2012 at 00:15 by: Dave Angel |
Possible thorium exposure! I wish I had known that TIG electrodes may be 'thoriated' before I ground one into separate electrod ... |
20-8-2012 at 08:28 by: Dave Angel |
Poor-man's spot welder success! Having searched the forum I see that the MOT spot welder is old news, but as a quick aside I just th ... |
20-8-2012 at 07:18 by: Dave Angel |
Free lab table Alas, a great shame as I have neither the room in my car for transport, nor my lab to install it, an ... |
20-8-2012 at 07:10 by: Dave Angel |
Chemistry Hackspace: Can it be done? It's good to see my first fellow brit on the map - [b]Hexavalent[/b]. I've never visited Anglesey my ... |
17-8-2012 at 14:36 by: Dave Angel |
Palladium (II) Chloride So, in order to carry out the synthesis of acetonitrile that I have propsed [url=http://www.sciencem ... |
17-8-2012 at 14:13 by: Dave Angel |
Palladium(II) catalysed dehydration of primary amides to nitriles Whilst there is another acetonitrile related thread going at the moment, a total synthesis post seem ... |
17-8-2012 at 13:38 by: Dave Angel |
Make Formic Acid Have a look at [url=http://www.erowid.org/archive/rhodium/chemistry/formic.acid.html]rhodium[/url] f ... |
14-8-2012 at 09:33 by: Dave Angel |
Vacuum pump I had the same concern with the waste of water with my first aspirator, and had to feed it with a ho ... |
11-8-2012 at 13:03 by: Dave Angel |
Vacuum pump There have been a couple of threads on vacuum pump advice recently, [url=http://www.sciencemadness.o ... |
11-8-2012 at 07:53 by: Dave Angel |
BBC RADIO 4, Nostalgia on chemistry sets broadcast. Nice find [b]MR AZIDE[/b]. Worth listening to if only because at one point the Cambridge Historian o ... |
11-8-2012 at 07:11 by: Dave Angel |
Toluene/water/ethanol azeotrope I'm currently working on ethanol production [b]mr.crow[/b] - are you looking at an immediately pract ... |
11-8-2012 at 06:17 by: Dave Angel |
Sodium! Thanks for the heads up [b]Bromic[/b]; on that back of it, I've decided to properly test the resista ... |
11-8-2012 at 05:24 by: Dave Angel |
What to do with tiny bits of Palladium wire? I've taken some better measurements now; the pieces are 0.5mm diameter and about 60, 80, and 50 mm l ... |
11-8-2012 at 05:15 by: Dave Angel |
H2S intoxication [rquote=255843&tid=10491&author=Zan Divine]The scarriest lab toxin to me is bis(chloromethyl ... |
2-8-2012 at 09:47 by: Dave Angel |
Purification of phosphorus -- treatment of WP burns [b]Endimion17[/b], I think you have seen that the pain that you have gone through to share these res ... |
30-7-2012 at 12:49 by: Dave Angel |
What to do with tiny bits of Palladium wire? I was sorting through my lab equipment this weekend and I came across many wonderful things I'd forg ... |
30-7-2012 at 12:10 by: Dave Angel |
Sodium! Castner progress this weekend: drilled out the crucible, and fitted the cathode, mesh and collection ... |
30-7-2012 at 11:54 by: Dave Angel |
is this a good vacuum pump? As I was describing in [url=http://www.sciencemadness.org/talk/viewthread.php?tid=20878#pid254770]an ... |
26-7-2012 at 11:23 by: Dave Angel |
Chemistry Hackspace: Can it be done? Nice idea [b]liquidlightning[/b]; you have my location.
So far, the 3 of us who have posted could ... |
26-7-2012 at 10:40 by: Dave Angel |
Sodium! Regarding [b]mineralman[/b]'s comment of chemicals becoming more difficult to aquire OTC or otherwis ... |
26-7-2012 at 09:49 by: Dave Angel |
Galvanize carbon fiber? My advice would be to get a hold of some pieces of CF weave and take it to a plater, ask them if the ... |
25-7-2012 at 10:43 by: Dave Angel |
Lithium and Sodium [rquote=252059&tid=20447&author=MR AZIDE]
Moral, look around for certain things, some plac ... |
21-7-2012 at 04:10 by: Dave Angel |