[Next Page] |
Carbon Foam Refractory Made From Bread It sure would be nice to have a kiln to do some of these experiments. Here's some metal containers I ... |
7-11-2016 at 09:29 by: Morgan |
Carbon Foam Refractory Made From Bread Yes, maybe something like parchment paper would do the trick to prevent sticking to the sides. Good ... |
6-11-2016 at 18:13 by: Morgan |
Carbon Foam Refractory Made From Bread I've some meter long quartz tubes with a mere 19 mm inside diameter/25 mm o.d. that I don't mind tra ... |
6-11-2016 at 17:10 by: Morgan |
Carbon Foam Refractory Made From Bread I was thinking bolete mushrooms would be a hopeful try at carbonizing because of the many dense litt ... |
6-11-2016 at 06:10 by: Morgan |
Carbon Foam Refractory Made From Bread Melba toast seems structurally sound, so maybe Melba toast would be something to try. If nothing els ... |
5-11-2016 at 14:00 by: Morgan |
Carbon Foam Refractory Made From Bread [rquote=466073&tid=70570&author=j_sum1][quote]I'd like to see a carbon foam that would be ai ... |
5-11-2016 at 08:46 by: Morgan |
Carbon Foam Refractory Made From Bread Tidbits and free associations
Maybe the structural strength could be improved by adding some chop ... |
5-11-2016 at 06:56 by: Morgan |
Cooked meat ate through aluminum foil! I had some qualms about putting the Reynolds information in quotes as if I shared their views. I don ... |
4-11-2016 at 17:40 by: Morgan |
Carbon Foam Refractory Made From Bread Seems like a very fine grain bread would make a stronger carbon foam, a dense bread with smaller por ... |
4-11-2016 at 08:41 by: Morgan |
Carbon Foam Refractory Made From Bread [rquote=465962&tid=70570&author=j_sum1]Let me throw out another possibility for this process ... |
3-11-2016 at 18:40 by: Morgan |
Cooked meat ate through aluminum foil! Tidbits
"According to the Reynold's Wrap website, "when aluminum foil comes in contact with a diffe ... |
3-11-2016 at 18:18 by: Morgan |
Fire, Ashes, Ammonia. Another variable
http://www.medhealthdaily.com/ammonia-smell-in-nose/ |
1-11-2016 at 10:09 by: Morgan |
Fire, Ashes, Ammonia. There're some clips on YouTube of cats attracted to green olives and in this article olive wood bowl ... |
1-11-2016 at 09:45 by: Morgan |
Fire, Ashes, Ammonia. Maybe if the wood had some beetles or grubs living in it that might contribute nitrogen over time. |
30-10-2016 at 06:29 by: Morgan |
Fire, Ashes, Ammonia. Another thought or remote outside possibility is if the washer was gunked up with that crap people l ... |
30-10-2016 at 05:19 by: Morgan |
Fire, Ashes, Ammonia. Maybe?
Applications
Destructive distillation of wood produces hundreds of compounds including ta ... |
29-10-2016 at 11:27 by: Morgan |
Platinum wire I wonder through some technology or brass tacks cleverness if you could subdivide the end of a piece ... |
27-10-2016 at 09:43 by: Morgan |
What to do with Teflon sewing thread? 550C I guess if you don't mind toxic gases.
http://catalog.cshyde.com/viewitems/ries-threads-cord ... |
21-10-2016 at 08:06 by: Morgan |
Platinum wire It seems like if platinized zirconia were enough to light methanol vapor without using a two step me ... |
20-10-2016 at 07:16 by: Morgan |
Platinum wire Thanks Fleaker, but I don't really need to know what my boats are made of at this time. I came acros ... |
18-10-2016 at 20:25 by: Morgan |
Platinum wire Thanks for the replies. It's not important, it was just a curiosity if iridium would give itself awa ... |
18-10-2016 at 07:52 by: Morgan |
Platinum wire Is there an easy way to to tell if platinum is alloyed with iridium or some other metal? The reason ... |
17-10-2016 at 10:09 by: Morgan |
Platinum wire Here's some thin stuff.
http://www.ebay.com/itm/Sigmund-Cohn-Wollaston-Wire-0-00001-dia-Pt-Core-One ... |
16-10-2016 at 18:18 by: Morgan |
Any interest in a palladium-based catalytic chemistry kit? Pd 1.25% on carbon rod bits, and Pd 0.5% on alumina pellets - the two on the right in both photos wi ... |
16-10-2016 at 12:02 by: Morgan |
Ammonium Hydroxide Since it was mentioned ammonia injection on the farm, this other use came to mind.
"In the United ... |
15-10-2016 at 11:27 by: Morgan |