Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. I've waited long enough to exhaust the 7 drops of formic acid that I added. After a week of electro ... |
17-3-2024 at 11:24 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Rough calcluation:
After doing several tests, the glacial acids tend to transfer as 48 drops for 1 ... |
12-3-2024 at 14:45 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. [file]101203[/file]
Obviously a crystalline precipitate is sticking to the electrode (-), this M ... |
11-3-2024 at 13:04 by: semiconductive |
What exactly is going on in this here molecule? [quote]so why does the calculations seem to fail for (1)? [/quote]
Hmm..
You're comparing a mole ... |
11-3-2024 at 01:20 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Experiment #507
See if conductivity can be increased by using combination of formic acid (stronger) ... |
9-3-2024 at 06:58 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Experiment completed: The color does slowly change to silvery nickel as the reaction proceeds. The ... |
6-3-2024 at 10:03 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Experiment #506.
I can't get NaCl to dissolve in acetic acid; but I notice that MgSO4 (epsom salt) ... |
4-3-2024 at 14:44 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. I see.
Well, whatever it is on the electrode; it *is* conductive and it does contain titanium.
It ... |
1-3-2024 at 15:36 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. For example, I mocked up two acetone molecules in the ENOL form and joined them with a divalent atom ... |
29-2-2024 at 16:23 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. [rquote=691287&tid=159974&author=Twospoons][rquote=689484&tid=159974&author=semicond ... |
29-2-2024 at 15:56 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Experiment #504. See if Acetone can complex divalent metals, such as nickel, and/or plate:
1 CC ... |
29-2-2024 at 14:05 by: semiconductive |
Inductor and capacitor for rectifier output filter I see.
Yes, the smoother the supply, the less time a typical transformer actually outputs energy ... |
17-2-2024 at 17:24 by: semiconductive |
Inductor and capacitor for rectifier output filter It usually is larger to have both a transformer and an inductor; because there is wasted space in ea ... |
16-2-2024 at 15:06 by: semiconductive |
Questions in electroplating [rquote=690755&tid=159939&author=clearly_not_atara]I'm confused? Isn't the anode supposed to ... |
8-2-2024 at 20:44 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Experiment #496 Calcium Butyrate + Ammonium nitrate in 99.97% IPA.
This is a partial success. ... |
23-1-2024 at 15:09 by: semiconductive |
Recrystallization, solubility of glacial acids. I'm just doing some physical chemistry experiments at the moment, and am curious about what is more ... |
2-1-2024 at 14:03 by: semiconductive |
Mantle no longer heating after spill silicone caulk mixed with ethyl-acetate can make a liquid that coats fiberglass circuit boards. I m ... |
19-12-2023 at 06:37 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. #494, mixed carboxylic glacial + ether + SO2 bearing molecule.
This is the pre-plate phase, where ... |
14-12-2023 at 11:34 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. It plates nicely at first, but the conductivity of the solution continues to rise; 10x.
The current ... |
5-12-2023 at 21:42 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Experiment #492 never plated. Fail. Continues to conduct electricity, with very slowly reducing cu ... |
4-12-2023 at 17:44 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Did some searching, and came across this:
[url=https://figshare.le.ac.uk/articles/journal_contrib ... |
3-12-2023 at 18:08 by: semiconductive |
cell design electrode surface, correct calculation Yes, it's the current that flows due to the meter impedance that is the problem.
Regular multimet ... |
3-12-2023 at 14:10 by: semiconductive |
cell design electrode surface, correct calculation I am not a chemist, and don't know much about nitrobenzene. I can't guide you there.
Having carbon ... |
2-12-2023 at 13:43 by: semiconductive |
cell design electrode surface, correct calculation Looks decent. Sanding pots is a bit of work.
I did a search for "porous cup", and found severa ... |
1-12-2023 at 11:51 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. I think I found another example.
Experiment #492, in order to get away from alkalai metals which ca ... |
30-11-2023 at 20:44 by: semiconductive |