KCLO3 by way of H2O + KCL [quote][i]Originally posted by Aqua_Fortis_100%[/i]
A little doubt ocurred now , all peoples says ... |
12-12-2007 at 10:00 by: Xenoid |
Cobalt Oxide Anodes [quote][i]Originally posted by dann2[/i]
@Xenoid. Is there still an MMO coating on the Ti electrode ... |
11-12-2007 at 21:30 by: Xenoid |
Cobalt Oxide Anodes Thanks 'spoons, I've finally got them apart. The epoxy never got to a "jellyish" state, it softened ... |
11-12-2007 at 18:17 by: Xenoid |
Cobalt Oxide Anodes [quote][i]Originally posted by Twospoons[/i]
@Xenoid: the way to attack epoxy is to get it nice and ... |
11-12-2007 at 17:06 by: Xenoid |
Cobalt Oxide Anodes [quote][i]Originally posted by dann2[/i]
One solution contained 2.5 moles CoCO3 6H2O per liter,
1 ... |
11-12-2007 at 17:00 by: Xenoid |
Cobalt Oxide Anodes [quote][i]Originally posted by chloric1[/i]
When you say that the anode only lasted 14 hours in the ... |
11-12-2007 at 15:56 by: Xenoid |
Homemade Rotary Shaker I would envisage something like a piece of chipboard, suspended from a metal frame by springs at the ... |
11-12-2007 at 15:33 by: Xenoid |
Chlorinator Disassembly Well, I decided to have a go at disassembling the chlorinator top! The blue plastic cover came off f ... |
11-12-2007 at 14:35 by: Xenoid |
KCLO3 by way of H2O + KCL @ Tim - if you are referring to my cell, I'm using that 48 amp halogen lighting transformer power su ... |
11-12-2007 at 12:20 by: Xenoid |
Cobalt Oxide Anodes [quote][i]Originally posted by dann2[/i]
When you say that a Chlorate cell is a 'piece of piss', ... |
11-12-2007 at 11:51 by: Xenoid |
KCLO3 by way of H2O + KCL Hashashan - I see you are still using "old fashioned" graphite (gouging rods), haven't you switched ... |
11-12-2007 at 11:25 by: Xenoid |
Cobalt Oxide Anodes [quote][i]Originally posted by dann2[/i]
have gone through about one gallon of 12% HCl keeping my ... |
11-12-2007 at 00:15 by: Xenoid |
Pottery Chemicals [quote][i]Originally posted by 12AX7[/i]
By admitting you cannot handle imperial measurements, you ... |
10-12-2007 at 23:38 by: Xenoid |
Other DECENT Forums? Look 4 posts up I guess, ScienceForums.Net |
10-12-2007 at 22:35 by: Xenoid |
Cobalt Oxide Anodes Hi guys,
Here's my latest Co oxide (spinel) anode, it's smoooooth, shiny and HARD.
Despite wha ... |
10-12-2007 at 22:13 by: Xenoid |
Cobalt Oxide Anodes [quote][i]Originally posted by Rosco Bodine[/i]
That's a good setup , but you could drill a 1/16" ... |
10-12-2007 at 14:31 by: Xenoid |
Cobalt Oxide Anodes [quote][i]Originally posted by dann2[/i]
I will be an extremly angry and bitter little man for a mo ... |
10-12-2007 at 14:03 by: Xenoid |
Cobalt Oxide Anodes WARNING NOTE:
Just a short note to anyone doing any Ti etching using hot / boiling conc. HCl.
I' ... |
9-12-2007 at 22:38 by: Xenoid |
Cobalt Oxide Anodes [quote][i]Originally posted by dann2[/i]
I am going to start up a Lithium Chlorate (or is it Perc ... |
9-12-2007 at 22:01 by: Xenoid |
Pottery Chemicals 1.1 Kg for $5, now that's good value....![:o](./images/smilies/shocked.gif)
The local pottery place here sells 500g for about NZ$5 ... |
9-12-2007 at 20:27 by: Xenoid |
Pottery Chemicals [quote][i]Originally posted by Xenoid[/i]
God - when will you Americans stop using all those loopy, ... |
9-12-2007 at 19:56 by: Xenoid |
Pottery Chemicals Err... 1/4lb is closer to 125g it's 2.2lb to the Kg
God - when will you Americans stop using all ... |
9-12-2007 at 18:05 by: Xenoid |
Cobalt Oxide Anodes I just went down to check on my remaining Co - nitrate concentrate which I had left in the fridge, a ... |
9-12-2007 at 17:11 by: Xenoid |
Cobalt Oxide Anodes Something else I was thinking about :
With the 4 coat baked spinel anode lasting (probably) at le ... |
9-12-2007 at 16:24 by: Xenoid |
Cobalt Oxide Anodes Well, my next move is back to baking! I'm very impressed with the way the Co oxide (spinel) is holdi ... |
9-12-2007 at 15:19 by: Xenoid |
[Next Page] |