The lead salts preparation thread!

Be aware that the gas liberation will cause a mist of liquid to come out of the container (like a ...
15-9-2011 at 14:52
by: dann2
Homeblown retort

The thinner the walls of the retort the less liable it will be to crack due to internal stresses i ...
11-9-2011 at 16:19
by: dann2
More on PbO2 electrodes

I had to abandon ship with my latest effort at coating a Tin Oxide coated Ti strip.
The Alpha (f ...
9-9-2011 at 13:48
by: dann2
piezoelectric bomb

Piezoelectric devices are used to produce EMP's (electromagnetic pulse) to knock out communication ...
7-9-2011 at 16:40
by: dann2
More on PbO2 electrodes
[rquote=220263&tid=2465&author=PolarSmokes]what about tin oxide on glass?[/rquote]

With a ...
7-9-2011 at 16:34
by: dann2
Elements for sale or trade

Is Bromine difficult to obtain. I know where a 500ml bottle of it is (Analar grade) and could per ...
7-9-2011 at 14:32
by: dann2
Tutorial for making a miniature chlorate cell
[rquote=221149&tid=14531&author=cyanureeves]
........ i used a s.steel pan with a propane t ...
6-9-2011 at 08:17
by: dann2
NaOH in the eyes

Not to trivialize the incident but link below shows 'just what the doctor ordered' (as they say)!! ...
5-9-2011 at 16:07
by: dann2
Be the first kid on the block with a hydrogen-fluorine torch
[rquote=220012&tid=17240&author=White Yeti] When it comes to welding, I'd rather have an AH ...
25-8-2011 at 14:32
by: dann2
Yum yum

I guess the quick acting poisons will not work for rats and the slow acting one's will not work fo ...
25-8-2011 at 14:16
by: dann2
More on PbO2 electrodes


All 'pin hole problems' have been solved with the arrival of the fault tolerant substrate
(MMO ...
25-8-2011 at 14:12
by: dann2
Ammonium Perchlorate Synthesis

@HB
Stop, stop you making me blush FFS!!!!!!!!!
21-8-2011 at 13:51
by: dann2
Bunch of shiite for sale.

Your location is.........
21-8-2011 at 13:44
by: dann2
MnO2 on graphite rod for electrolisis of chlorate/bromate
Xenoid tried putting MnO2 onto gouging rods with little success.
See:
http://sciencemadness.org/ta ...
21-8-2011 at 13:41
by: dann2
Ampouling volatile liquids

I have a bottle with a Teflon washer inside the lide which will do the job I presume.

Titanium ...
19-8-2011 at 11:41
by: dann2
Ammonium Perchlorate Synthesis
It's simply an error in the book. Jade Ledgard mush have been reading it too............

http://o ...
16-8-2011 at 14:06
by: dann2
Tutorial for making a miniature chlorate cell
[rquote=219009&tid=14531&author=cyanureeves].........battery crud. i have gotten as far as m ...
15-8-2011 at 05:32
by: dann2
Thoughts On Anodes

I have never tried SnCl2 with BiCl3, only ever used/tried SnCl4:5H2O

I could never get anything ...
9-8-2011 at 17:29
by: dann2
Thoughts On Anodes

Swedes blog can be had on APC forums:
You will neen to subscribe and go to a post of Swede and a ...
9-8-2011 at 13:54
by: dann2
Help finding epoxy to seal mmo anodes in housing

"What I am trying to find out is how to seal the edges of my mmo material that have been sheared." ...
9-8-2011 at 13:51
by: dann2
A small scale fluorine generator
Nice one. This should cure my mother in law problems.
9-8-2011 at 07:43
by: dann2
Thoughts On Anodes

Any experiments I have done up to now have been done using homemade Bismuth Trichloride (BiCl3:3H2 ...
9-8-2011 at 07:40
by: dann2
Help finding epoxy to seal mmo anodes in housing

I have used stuff from the car accessory shop. It is polyester resin and it is used in conjunction ...
9-8-2011 at 07:36
by: dann2
How many research papers are freely available? - August 01, 2011

I'll second that!
8-8-2011 at 12:58
by: dann2
Pretty Pictures (1)

Some Oxide spots on Nb by placing drops of KCl solution on a Nb sheet and connecting the sheet to ...