Search |
[Next Page] |
Solvent ideas needed. Theres a petroleum based solvent product here in the US and Canada called "Goo Gone". It's yellowis ... |
7-4-2008 at 15:36 by: Saerynide |
Galvanised Iron LPG tank [quote][i]Originally posted by Panache[/i]
Finally the steam coming out of it still smells like a l ... |
7-4-2008 at 15:29 by: Saerynide |
Pt (jewelry) Ir/Rh? Don't get Rh. Rh is used too often in cheap costume jewelry (like base metal plated in Rh or Cr) to ... |
7-4-2008 at 14:55 by: Saerynide |
College Interview I neved did interviews for college (but I did talk about my passion for chemistry in my application ... |
7-4-2008 at 14:11 by: Saerynide |
Mettler H10 W00T. After 3 hours of fiddling with lasers and leds, I got the optical display working. For some ... |
31-3-2008 at 05:47 by: Saerynide |
Mettler H10 So, my H20T came in pieces, as expected. I managed to put all the weights back where they are suppo ... |
29-3-2008 at 13:09 by: Saerynide |
Mettler H10 Awesome! Thanks Can't wait for the scale to get here now |
20-3-2008 at 22:19 by: Saerynide |
Mettler H10 After being MIA for 2 years, I am back! Its nice to see how so many of you guys are still here
... |
19-3-2008 at 16:03 by: Saerynide |
fuckin plastic piece of shit hoses Wow. That sucks. Glad you're ok.
Btw, fire the bastard. |
13-6-2006 at 03:44 by: Saerynide |
Spark Gap Tesla Coil Thats awesome guys |
10-7-2005 at 07:35 by: Saerynide |
Microwave-made Nitric Acid Sounds wonderful if it works as intended |
30-6-2005 at 11:08 by: Saerynide |
Bromine Source and Synthesis Nice Looking forward to reading more about it. |
11-6-2005 at 01:59 by: Saerynide |
Woo hoo, I built a working ball mill!!! What was that all about?
Anyways, I look forward to seeing your pics evil_lurker |
28-5-2005 at 05:00 by: Saerynide |
How do I store I2? Can I2 be stored under water since its insoluble? |
9-5-2005 at 02:05 by: Saerynide |
Merck Index problem This probably sounds really stupid, but I can't figure out how to get out of the Structure Draw ... |
8-5-2005 at 04:54 by: Saerynide |
Green arrow thing Yeah, I see the new stickies |
6-5-2005 at 07:53 by: Saerynide |
a simple equation... If you look at the standard reduction potential of the MnO4- in acid to Mn2+, it is 1.51 V the pote ... |
2-5-2005 at 07:38 by: Saerynide |
a simple equation... first one is
8 H2SO4 + 2 KMnO4 + 10 FeSO4 --> 2 MnSO4 + K2SO4 + 5 Fe2(SO4)3 + 8 H2O
The rest ... |
2-5-2005 at 07:24 by: Saerynide |
a simple equation... KNO4 and Fe2SO4 do not exist.
Do you mean iron (II) sulfate FeSO4? |
2-5-2005 at 04:40 by: Saerynide |
Green arrow thing I can't figure out what the little green box with a white arrow next to certain threads mean. ... |
23-4-2005 at 00:30 by: Saerynide |
Introduction!!! (Hello Y'all!!!) What's it like to be a hazmat manager? |
20-4-2005 at 02:16 by: Saerynide |
Rotting Meat - a graphical treatise.... Interesting I think I'm gonna barf soon though |
19-4-2005 at 03:40 by: Saerynide |
Melting Lithium Wont it thermite with the magnesium oxide? |
12-4-2005 at 06:00 by: Saerynide |
Subscript days are numbered? I can't be bothered to use em. I find myself forgetting to write them in school even |
8-4-2005 at 02:24 by: Saerynide |
Formulas against ants... Just being nit picky, but dont you mean, [i]formulas against ants[/i]? |
4-4-2005 at 07:39 by: Saerynide |