(Neutron detector) Melting Lithium fluoride into bigger, clean lumps- no it'm actually not tied to it at all, i was just asked to help.
the idea with the nuts and bolt ... |
14-2-2018 at 09:48 by: Naaaan |
(Neutron detector) Melting Lithium fluoride into bigger, clean lumps- Ok i got more information now, talking to the ppl i am working with:
They want the Li[sup]+[/sup] ... |
14-2-2018 at 03:39 by: Naaaan |
(Neutron detector) Melting Lithium fluoride into bigger, clean lumps- In certain, thick enough test tubes, you can melt LiF (tried it also with NaCl, which has a slightly ... |
13-2-2018 at 10:59 by: Naaaan |
(Neutron detector) Melting Lithium fluoride into bigger, clean lumps- Hi there,
since i have been more of an metal-organic (catalyst-design) chemist, i don't know much ... |