Search |
RMS Battery Update Greatings its been a while since the group talked about Robert Murray Smith batteries. So I thought ... |
11-11-2018 at 16:00 by: Geekineer |
Baseline Cell Here is the 'recipe' and test results for my base line cell.
1. Size: two discs 1.5" diameter co ... |
30-12-2016 at 04:38 by: Geekineer |
The Robert Murray-Smith Battery WGTR
From your last post, I'm trying to understand the carbon black component.
There is research ... |
16-12-2016 at 06:18 by: Geekineer |
RMS Vid on Battery Strategy Dec 14, 2016 Note - there is typically as much info if you read all (hundreds) of comments on the videos as oppos ... |
15-12-2016 at 14:16 by: Geekineer |
The Robert Murray-Smith Battery WGTR - the vid I referred to is titled "Structured Carbon Battery" see segment 1.5 minutes to 3.5 m ... |
15-12-2016 at 08:51 by: Geekineer |
The Robert Murray-Smith Battery Hi WGTR
In RMS lastest vid he shows a cell concept without separate current collector - but part of ... |
14-12-2016 at 06:08 by: Geekineer |
RMS latest video In Robs latest vid - about 2 weeks ago - he seems to abandon his graphene ink on grafoil electrodes, ... |
11-12-2016 at 15:36 by: Geekineer |
The Robert Murray-Smith Battery Maybe the spreadsheet is the best way to keep track of videos, recipes, suppliers etc.
I've made ... |
10-12-2016 at 08:43 by: Geekineer |
RMS EESD Work Outline Hello - been following RMS for a while - thought I'd post a rough outline here and with some of this ... |
7-12-2016 at 15:58 by: Geekineer |
Testing Ionic Membranes What I have now is just that - a test cell with replaceable membrane. Any suggestions on the electr ... |
23-12-2015 at 12:49 by: Geekineer |
3D printing ionic membranes What about taking the milled ionic resins and extruding it into 1.75mm filament for 3D printing - no ... |
21-12-2015 at 13:59 by: Geekineer |
Testing Ionic Membranes I need to measure the relative (not calibrated or absolute) performance of anion membranes. Looking ... |
21-12-2015 at 13:33 by: Geekineer |