It’s not critical so long as you have a slight excess of acid. You will be adding more iron into solution anyways.

As long as metallic iron is present ferric will be reduced to ferrous in acid solution




Fellow molecular manipulator
View user's profile View All Posts By User
chloric1
International Hazard
*****




Posts: 1071
Registered: 8-10-2003
Location: GroupVII of the periodic table
Member Is Offline

Mood: Stoichiometrically Balanced

[*] posted on 31-1-2023 at 16:27


Quote: Originally posted by woelen  
Recovering oxidized iron(II) sulfate is very difficult and is not worth the effort. If you want an iron(II) salt, then next time I would purchase Mohr's salt, Fe(NH4)2(SO4)2.12H2O. Mohr's salt is MUCH more stable in air than ferrous sulfate. It is not so easily oxidized.


Sorry but no. It’s so easy. I have purchased “copperas” from a fertilizer co-op store, took it home, and made up 20% sulfuric acid solution added the brownish yellow iron salt and boiler with regular nails for about an hour or two and let it cool and got beautiful blue green crystals