Loading [MathJax]/jax/output/HTML-CSS/fonts/TeX/fontdata.js
Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Molybdates + photos
samarium14
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 20-3-2021 at 02:24
Molybdates + photos


Hi. Today i made some metals molybdates. There are nickel copper and cobalt molybdates and THERE are manganese and some kind of gallium molybdate. I think it would be better if information on all types of molybdates were collected and not scattered at all points in the forum. I only have these molybdates at the moment, but I will definitely make others in the future.

received_767476087243253.jpeg - 346kB




View user's profile View All Posts By User
samarium14
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 20-3-2021 at 02:27


Comparison of Ni, Cu and Co tungstates with color



View user's profile View All Posts By User
Lion850
National Hazard
****




Posts: 517
Registered: 7-10-2019
Location: Australia
Member Is Offline

Mood: Great

[*] posted on 20-3-2021 at 02:40


Very nice Vano. I do have MoO3; I must try some.
View user's profile View All Posts By User
samarium14
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 20-3-2021 at 02:48


Thanks. Good luck.



View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6361
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 20-3-2021 at 03:44


I still have some ammonium molybdate to give away (as of today's date.) U2U me if interested.
View user's profile View All Posts By User
Lion850
National Hazard
****




Posts: 517
Registered: 7-10-2019
Location: Australia
Member Is Offline

Mood: Great

[*] posted on 21-3-2021 at 01:48


Hi j_sum1 thanks for the offer, I also have that in the shed. The reason I'd rather use the molybdic acid MoO3 as a starting material is simply because I have some 500g of it.
View user's profile View All Posts By User
samarium14
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 21-3-2021 at 04:09


Lion850 I just wonder where you bought 500g MoO3?



View user's profile View All Posts By User
Lion850
National Hazard
****




Posts: 517
Registered: 7-10-2019
Location: Australia
Member Is Offline

Mood: Great

[*] posted on 21-3-2021 at 17:43


Vano there is a local chemical supplier that is happy to sell some stuff to hobbyists, and to let go of old stock cheap. The MoO3 came from him.
View user's profile View All Posts By User
samarium14
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 21-3-2021 at 21:51


It is wonderful. Perhaps the seller knows the chemistry, I have a problem with the fact that most of them do not know the chemistry and just can not find the necessary compound. Chemicals that I have I have seen too many of them by chance, including sodium molybdate. If they knew chemistry I would have a lot of very rare substances today. But once more than half a kilo of Phosphotungstic acid was given to me because he did not know what to use it for, And many other substances as well.



View user's profile View All Posts By User