Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Weird precipitate (tin-carbonate?)
dome13
Harmless
*




Posts: 30
Registered: 29-6-2019
Location: Hungary
Member Is Offline


[*] posted on 25-2-2021 at 08:08
Weird precipitate (tin-carbonate?)


Hello!
I am currently synthetising p-aminobenzoic acid from p-nitrobenzoic acid. The reducing agent was SnCl2 x 2 H2O in absolute ethanol. After refluxing I diluted with water and basified with NaHCO3. This caused a white precipitate, tin(IV)-carbonate. After vacuum filtration I placed the filtrate in a warm place in order to dry. On the next day I was suprised, that the volume was drastically reduced and it got a yellow-amber like color. It is a side note what I found interesting: immeditially after filtration, it has a physical properties like vaseline or cold fat.
So, my quiestion is, is this how tin(IV)-carbonate supposed to look like after drying, or is it something else?

IMG_20210225_160658.jpg - 2.9MB
View user's profile View All Posts By User
njl
National Hazard
****




Posts: 609
Registered: 26-11-2019
Location: under the sycamore tree
Member Is Offline

Mood: ambivalent

[*] posted on 25-2-2021 at 08:19


I don't think tin carbonates are stable and instead decompose into oxides. You probably have a tin oxide/hydroxide contaminated with your target compound and precursor.



Reflux condenser?? I barely know her!
View user's profile View All Posts By User
dome13
Harmless
*




Posts: 30
Registered: 29-6-2019
Location: Hungary
Member Is Offline


[*] posted on 26-2-2021 at 09:47


It seems to reasonable. Thank you for your answer!
View user's profile View All Posts By User
Amos
International Hazard
*****




Posts: 1406
Registered: 25-3-2014
Location: Yes
Member Is Offline

Mood: No

[*] posted on 26-2-2021 at 17:11


I don't think tin is oxidized all the way to the +4 oxidation state; I believe you have tin(II) hydroxide, which often forms a gel, colored brown with oxidized impurities from your p-aminobenzoic acid.
View user's profile View All Posts By User
Boffis
International Hazard
*****




Posts: 1884
Registered: 1-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 27-2-2021 at 01:36


Its possible that you have incomplete reduction and some hydroazobenzoic acid (white)has formed which then oxidizes to azobenzoic acid (orange-red), on exposure to air, mixed in with the hydrated tin IV oxide.
View user's profile View All Posts By User
dome13
Harmless
*




Posts: 30
Registered: 29-6-2019
Location: Hungary
Member Is Offline


[*] posted on 27-2-2021 at 05:15


Thank you for your replies!
The reduction indeed was not completed, I got about half of the expected yield.
On the next step, where I made benzocaine, the solution didn't clear up fully on reflux. Altough I got a good yield, the melting point was way too high compared to literature. The anesthetic effects was negligible too.
I planning to do the synthesis again and try to avoid these little mistakes.

[Edited on 27-2-2021 by dome13]
View user's profile View All Posts By User