Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Chart Comparing Various Fluoropolymers
thermochromic
Harmless
*




Posts: 17
Registered: 17-1-2018
Member Is Offline

Mood: No Mood

[*] posted on 21-8-2020 at 23:33
Chart Comparing Various Fluoropolymers


Ran across this earlier thought some other people may find it informational...







[Edited on 22-8-2020 by thermochromic]
View user's profile View All Posts By User
macckone
Dispenser of practical lab wisdom
*****




Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 22-8-2020 at 08:34


Wish that chart had viton, but there are bunch of types for viton.
View user's profile View All Posts By User
Phosphor-ing
Hazard to Others
***




Posts: 248
Registered: 31-5-2006
Location: Deep South, USA
Member Is Offline

Mood: Inquisitive

[*] posted on 22-8-2020 at 09:54


https://www.viton.com/en/-/media/files/viton/viton-selection...

A lot of information here but there are some Viton charts here.




"The nine most terrifying words in the English language are: 'I'm from the government and I'm here to help.'" -Ronald Reagan
View user's profile View All Posts By User
macckone
Dispenser of practical lab wisdom
*****




Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 22-8-2020 at 10:05


Quote: Originally posted by Phosphor-ing  
https://www.viton.com/en/-/media/files/viton/viton-selection...

A lot of information here but there are some Viton charts here.


Thanks posting the pdf here in case the link vanishes.

Attachment: viton selection guide.pdf (104kB)
This file has been downloaded 278 times

View user's profile View All Posts By User