[*] posted on 19-2-2011 at 09:54
SnI4 and TiI4


today i made this experiment : http://81.207.88.128/science/chem/exps/SnI4/index.html

but with some change , i use CHCl3 instead of CS2 ( i made it frome acetone + sodium hypochlorite 4%). i boil it with a tube outside the lab.

now i want to repeat this experiment but in the place of making tin tetraiodide , i want to make titanium tetraiodide ( if it work i will made a youtube video about it , tomorow).

solvent: 95-96% CHCl3
iodine 95-98%
and 1/4 to 1/2inch pellet of 99.999% titanium
but the problem is i need titanium powder for this reaction , i tried to grind it with a file but it is nearly impossible.



thanks!!

[Edited on 19-2-2011 by plante1999]

[Edited on 19-2-2011 by plante1999]

[Edited on 19-2-2011 by plante1999]

[Edited on 19-2-2011 by plante1999]

[Edited on 19-2-2011 by plante1999]

[Edited on 20-2-2011 by plante1999]
View user's profile View All Posts By User
plante1999
International Hazard
*****




Posts: 1936
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 19-2-2011 at 17:05


solvent: 95-96% CHCl3
iodine 95-98%
and titanium powder

Finally I grind the titanium mecanicly with aluminia oxide sand paper.


the powder was very fine and i ad the conssentred iodine solution ( in CHCl3 ) to it at temperature piece and no reation occured ( not like the Sn + I2 reaction , arroun 30 second and it is finish) so i heated it , the titanium make tiny effervescence and nothing more after 2 hour wath do you thing do i need to heat 60degree C with reflux for 1-2hour? or ad a catalist? Al powder ( 2Al + 3I2 -> 2AlI3 --------------------- 3 Ti + 4 AlI3 = 3 TiI4 + 4 Al and the al could be filtered)?


[Edited on 20-2-2011 by plante1999]
View user's profile View All Posts By User
hkparker
National Hazard
****




Posts: 601
Registered: 15-10-2010
Location: California, United States
Member Is Offline

Mood: No Mood

[*] posted on 19-2-2011 at 18:39


Thanks for drawing my attention to this, hopefully ill do a video on SnI4 for my youtube channel soon.

As for your reaction I'm not so sure it will react. You could try to reflux it but how are you sure iodine solution will attack titanium?, a pretty corrosion resistant metal. As for it displacing aluminum, check the reactivity series. I always though of titanium as pretty noble but it could just be passivation that prevents reactions. Let me know how it goes, cool stuff.




My YouTube Channel

"Nothing is too wonderful to be true if it be consistent with the laws of nature." -Michael Faraday
View user's profile Visit user's homepage View All Posts By User
plante1999
International Hazard
*****




Posts: 1936
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 19-2-2011 at 18:50


titanium is a prety reactive element (think pyro) but the dioxide layer protect it ,brauer said that Ti react with I2 , fast at 200degree C. for the al reactivity sery , brauer said a method with al/ti alloy in iodine solution.

[Edited on 20-2-2011 by plante1999]
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 20-2-2011 at 07:52


Quote: Originally posted by hkparker  
Thanks for drawing my attention to this, hopefully ill do a video on SnI4 for my youtube channel soon.

As for your reaction I'm not so sure it will react. You could try to reflux it but how are you sure iodine solution will attack titanium?, a pretty corrosion resistant metal. As for it displacing aluminum, check the reactivity series. I always though of titanium as pretty noble but it could just be passivation that prevents reactions. Let me know how it goes, cool stuff.


Forget the potential series for a minute: that’s very useful for electrochemistry in watery solution but it says very little about reactions like this one.

Plante is correct in saying that titanium is in fact a very reactive metal: it can be made to burn in air for instance. But it passivates very efficiently, protecting the metal against corrosion. Commercial Ti metal dissolves fairly easily in hot conc. HCl, to TiCl3 (aq)…

In the Van Arkel and De Boer crystal bar method, very pure Zr or Ti is obtained by decomposing the resp. tetra iodides (ZrI4 or TiI4) on a hot filament (about 1200 C). New, pure ZrI4 or TiI4 is constantly formed in situ and constantly decomposed to very pure metal at the filament (the I2 is thus constantly being recycled).

TiI4 is a non-ionic material albeit with probably a sizeable heat of formation, which drives the reaction Ti + 2I2 === > TiI4.

I feel TiI4 probably can be made similar to SnI4 but obtaining or making powdered Ti is hard.
View user's profile View All Posts By User
plante1999
International Hazard
*****




Posts: 1936
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 20-2-2011 at 08:17


after testing the Ti react with I2 when refluxed. I will post a video later.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 20-2-2011 at 09:26


Quote: Originally posted by plante1999  
after testing the Ti react with I2 when refluxed. I will post a video later.


Yes, you do that.
View user's profile View All Posts By User
plante1999
International Hazard
*****




Posts: 1936
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 20-2-2011 at 17:29


here a qick review of the video that i will made . (this is only a 14 day trial)I will re-try to make it in 14day ( I REALY NEED TO IMPROUVE MY WAY TO MAKE TiI4). also it as some missing parts.
as you can see at the end it is not like I2 its is dark violet brown-red , with some heating no I2 vapor form but a very dense darck red-brown fume are formed at high temperature)

<iframe sandbox title="YouTube video player" width="480" height="390" src="http://www.youtube.com/embed/JX1jCrbdivM" frameborder="0" allowfullscreen></iframe>
View user's profile View All Posts By User
plante1999
International Hazard
*****




Posts: 1936
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 20-2-2011 at 18:22


sorry for the double post.

here how i made my solvent , i take very long time to make an usable amount of solvent. I know it is the same music but the first video will be delleted in 14day , so....

<iframe sandbox title="YouTube video player" width="480" height="390" src="http://www.youtube.com/embed/u8vfuqzG8l8" frameborder="0" allowfullscreen></iframe>
View user's profile View All Posts By User
hkparker
National Hazard
****




Posts: 601
Registered: 15-10-2010
Location: California, United States
Member Is Offline

Mood: No Mood

[*] posted on 20-2-2011 at 23:16


I did a video on SnI4 if anyone wants to see, its on my channel.



My YouTube Channel

"Nothing is too wonderful to be true if it be consistent with the laws of nature." -Michael Faraday
View user's profile Visit user's homepage View All Posts By User
Jor
National Hazard
****




Posts: 950
Registered: 21-11-2007
Member Is Offline

Mood: No Mood

[*] posted on 21-2-2011 at 05:16


Plante1999, I can't see your video on TiI4, because it is private.
View user's profile View All Posts By User
plante1999
International Hazard
*****




Posts: 1936
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 21-2-2011 at 05:21


i will change that take note this is just a report of the experiment not the final guide.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 21-2-2011 at 08:36


Yes, you seem to have made TiI4. But your claim of seeing TiI4 vapour is dubious: it has a boiling point of 377 C.

Have you tried hydrolysing some of it?

[Edited on 21-2-2011 by blogfast25]
View user's profile View All Posts By User
plante1999
International Hazard
*****




Posts: 1936
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 21-2-2011 at 08:46


i will do tonight. 99 post!!
View user's profile View All Posts By User
plante1999
International Hazard
*****




Posts: 1936
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 21-2-2011 at 09:51


sorry for the double post
this ismy 100th post!

my hot plate haet to 900degree C so....but with amiante sheat it it to 500 degree c.

in 13 day i will improuve my methode , i am in working of a self made ( glass bowing with already made glass part) appartus for making TiI4 , TiCl4 and many other inorganic titanium syntesis.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 21-2-2011 at 14:03


'amiante' (wonderful word!) = asbestos.
View user's profile View All Posts By User
plante1999
International Hazard
*****




Posts: 1936
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 21-2-2011 at 14:06


sorry for the mistake . i hydrolise te TiI4 and after 2minute a ligth yellow solution is formed i will lets it hydrolise more time.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 21-2-2011 at 14:39


Interesting test could be to add some NaF solution to TiI4, you should get TiF4! Dry mixing TiI4 with NaF should also yield TiF4 with some mild heating: TiI4 + 4 NaF ---> TiF4 + 4 NaI, driven by the higher HoF of TiF4.
View user's profile View All Posts By User
plante1999
International Hazard
*****




Posts: 1936
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 21-2-2011 at 15:22


yes this woul be a good idee but in wath solvent do you think i should use?
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 22-2-2011 at 10:22


Try heating an intimate dry mix. TiF4 is highly prone to hydrolysis (HF alert!) so separting the NaI and TiF4 may be difficult unless there exists an aprotic solvent for NaI...
View user's profile View All Posts By User
Lambda-Eyde
National Hazard
****




Posts: 860
Registered: 20-11-2008
Location: Norway
Member Is Offline

Mood: Cleaved

[*] posted on 22-2-2011 at 11:49


Acetone?
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 22-2-2011 at 12:55


If NaI is soluble in acetone (is it?) then heating an intimate mix of TiI4 with NaF in a closed reactor, followed by leaching out the NaI with acetone could indeed be a way to make small amounts of TiF4 (quite a nasty substance from what little I've read about it...)

[Edited on 22-2-2011 by blogfast25]
View user's profile View All Posts By User
Lambda-Eyde
National Hazard
****




Posts: 860
Registered: 20-11-2008
Location: Norway
Member Is Offline

Mood: Cleaved

[*] posted on 22-2-2011 at 13:07


Well, it's the basis for the Finkelstein reaction, so that would make sense.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 22-2-2011 at 13:38


Interesting Lambda-Eyde, never heard of that one before...
View user's profile View All Posts By User
plante1999
International Hazard
*****




Posts: 1936
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 22-2-2011 at 16:50



This is a plan of the apparatus i will make for making majority of Ti and Zr compound (i made just Zr and Ti compound. it will cost arround 5dollar us , for all glass reflux it is cheap.

[Edited on 23-2-2011 by plante1999]