[*] posted on 10-9-2006 at 16:10
Anhydrous AlCl3??


Hey everyone.
I want to make anhydrous aluminum chloride to use as a catalyst in a reaction i am working on.
I have found a procedure which requires passing dry HCl over heated aluminum powder....

http://designer-drugs.com/pte/12.162.180.114/dcd/chemistry/a...

Does anyone have any experience of this? Are there any problems which may occur with this method? Would Cl2 work better than HCl?

I was also wondering whether powdering kitchen foil would be a suitable source for the Al powder.. in other words, how pure is aluminum foil?... do they use some sort of alloy or is it pure enough for this reaction.

Any help will be very much appreciated...

[Edited on 11-9-2006 by sonogashira]
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 10-9-2006 at 16:41


Foil is something like 98% pure, the remainder is mostly iron and silicon IIRC.

If you wanted to be sure, you could sublimate the AlCl3 I suppose.

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
unionised
International Hazard
*****




Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 11-9-2006 at 10:46


FeCl3 and SiCl4 are reasonable substitues for AlCl3 in many cases (at least if you are just using it as a catalyst). Purification might be more trouble than it's worth.
Cl2 and HCl both work and they are both nasty to work with. The reaction with HCl gives rise to H2 which complicates things because it's flammable.
What experience do you have with this sort of reaction?
View user's profile View All Posts By User
Maja
Hazard to Others
***




Posts: 143
Registered: 27-2-2006
Member Is Offline

Mood: No Mood

[*] posted on 11-9-2006 at 11:04


I faced with that kind of problem ,because of AlCl3.. I just bought 100gr of Anhydrous AlCl3 and then made much more myself by bubbling HCl gas thru inert solvent where Al powder was suspended. You need to initiate reaction with small amount of AlCl3, otherwise it won't work. Now I would make small amount of AlCl3 myself. I don't know for what you will use that, but you can substitute it with FeCl3 or SiCl4 as unionised said. Thanks.
View user's profile View All Posts By User
sonogashira
National Hazard
****




Posts: 555
Registered: 10-9-2006
Member Is Offline

Mood: No Mood

[*] posted on 11-9-2006 at 11:06


Do you not think that the product will be reasonably pure? Perhaps if i found a better source of Al than Al foil would that solve the purity concerns?.... Do you see the problem arising from the contaminants in the aluminum or does the process itself lead to an impure product?...
The flammability issue is not a huge concern, i will take suitable precautions.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 11-9-2006 at 12:41


The product will be pretty pure and the impurities probably won't matter much for most things.
View user's profile View All Posts By User
Nick F
Hazard to Others
***




Posts: 439
Registered: 7-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 11-9-2006 at 13:01


Does the procedure not involve sublimation itself? If so, that would purify it. I haven't read the procedure, because I'm at a friend's house and he might not want designer-drugs.com on his computer....
But as unionised said, iron and silicon impurities shouldn't matter.
I'd prefer to use HCl than Cl2. Hydrogen isn't a problem to deal with, HCl is a bit less nasty, and it's easier to make anhydrous.
View user's profile View All Posts By User
sonogashira
National Hazard
****




Posts: 555
Registered: 10-9-2006
Member Is Offline

Mood: No Mood

[*] posted on 11-9-2006 at 13:03


Thanks for your help.... Will give it a try and report back.
View user's profile View All Posts By User
sonogashira
National Hazard
****




Posts: 555
Registered: 10-9-2006
Member Is Offline

Mood: No Mood

[*] posted on 11-9-2006 at 13:07


"Does the procedure not involve sublimation itself?"

It basically involves passing a stream of dry HCl over heated Al powder in a tube.
View user's profile View All Posts By User
hodges
National Hazard
****




Posts: 525
Registered: 17-12-2003
Location: Midwest
Member Is Offline


[*] posted on 11-9-2006 at 13:34


One idea which I have never heard proposed before but seems like it might work would be to react hexachloroethane (C2Cl6, available as a pyrotechnic supply) with aluminum powder in a sealed container. This should be self-sustaining once started; experiment starting with a small amount of reactants on the size of the aluminum particles to get a rate that is not too fast.

You will end up with some carbon as well but might not be a problem; depending on your reaction you could filter it off later.

Hodges
View user's profile View All Posts By User
Nicodem
Super Moderator
*******




Posts: 4230
Registered: 28-12-2004
Member Is Offline

Mood: No Mood

[*] posted on 11-9-2006 at 14:15


Quote:
Originally posted by hodges
One idea which I have never heard proposed before but seems like it might work would be to react hexachloroethane (C2Cl6, available as a pyrotechnic supply) with aluminum powder in a sealed container. This should be self-sustaining once started; experiment starting with a small amount of reactants on the size of the aluminum particles to get a rate that is not too fast.

You will end up with some carbon as well but might not be a problem; depending on your reaction you could filter it off later.

Hodges


https://sciencemadness.org/talk/viewthread.php?tid=1542#pid3...




…there is a human touch of the cultist “believer” in every theorist that he must struggle against as being unworthy of the scientist. Some of the greatest men of science have publicly repudiated a theory which earlier they hotly defended. In this lies their scientific temper, not in the scientific defense of the theory. - Weston La Barre (Ghost Dance, 1972)

Read the The ScienceMadness Guidelines!
View user's profile View All Posts By User
matei
Hazard to Others
***




Posts: 205
Registered: 16-9-2006
Member Is Offline

Mood: No Mood

[*] posted on 16-9-2006 at 14:23


In "Vogel's Practical Organic Chemistry" you can find the procedure for obtaining anhydrous AlCl3 by sublimation. This should be sufficiently dry for catalytic purposes.
View user's profile View All Posts By User
sonogashira
National Hazard
****




Posts: 555
Registered: 10-9-2006
Member Is Offline

Mood: No Mood

[*] posted on 16-9-2006 at 14:44


Thanks a lot matei!!
I have the 5th edition... I had a little look but couldn't find it. Could you give me a page number (or say what section it is under if you have a different edition).. Many thanks for your help!!
View user's profile View All Posts By User
ethan_c
Hazard to Others
***




Posts: 104
Registered: 5-6-2006
Member Is Offline

Mood: No Mood

[*] posted on 16-9-2006 at 15:41


Quote:
Originally posted by unionised
The product will be pretty pure and the impurities probably won't matter much for most things.


Look at the website he is sourcing from. Although I guess if you're dumb enough to be making drugs either to sell or for your own consumption, impurities are probably the least of your worries.
View user's profile View All Posts By User
sonogashira
National Hazard
****




Posts: 555
Registered: 10-9-2006
Member Is Offline

Mood: No Mood

[*] posted on 16-9-2006 at 15:52


wtf??
Who said anything about making drugs... If you can find another anhydrous AlCl3 synthesis on the internet i would be very interested..
Please don't be so judgemental...
View user's profile View All Posts By User
ethan_c
Hazard to Others
***




Posts: 104
Registered: 5-6-2006
Member Is Offline

Mood: No Mood

[*] posted on 16-9-2006 at 18:52


Quote:
Originally posted by sonogashira
wtf??
Who said anything about making drugs... If you can find another anhydrous AlCl3 synthesis on the internet i would be very interested..
Please don't be so judgemental...


You're right, a google search did turn that particular procedure up immediately. However, it took 35 seconds fliping pages to find out… that synthesis is copied word for word from Brauer. The internet can be helpful, but I would personally much prefer actual literature to a site like that.
View user's profile View All Posts By User
Nicodem
Super Moderator
*******




Posts: 4230
Registered: 28-12-2004
Member Is Offline

Mood: No Mood

[*] posted on 16-9-2006 at 23:00


Quote:
Originally posted by ethan_c
… that synthesis is copied word for word from Brauer. The internet can be helpful, but I would personally much prefer actual literature to a site like that.

All Rhodium pages have references to where the procedure was taken from and this one is no exception (check the end of the page). Among the hundreds pages, there are only a couple of errors which can be easily spotted by checking the original papers.

So, I do agree that one should take the information from the original literature, but more because there is often some additional information there that can be of use. Otherwise, the Rhodium's archive is pretty much trustworthy for the part that is the transcription from academic literature as well as most (but not all) of the part that originated from amateur experimenters.

I know several friends that work in academic laboratories that sometimes source references and procedures from that incredibly rich archive. Not surprisingly, given that it takes a couple of seconds to check the net when compared to going to the library for a reference search and then looking up for the papers.

PS: What has AlCl3 to do with drugs?




…there is a human touch of the cultist “believer” in every theorist that he must struggle against as being unworthy of the scientist. Some of the greatest men of science have publicly repudiated a theory which earlier they hotly defended. In this lies their scientific temper, not in the scientific defense of the theory. - Weston La Barre (Ghost Dance, 1972)

Read the The ScienceMadness Guidelines!
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 17-9-2006 at 11:19


Whether the chemicals he hopes to produce are drugs or not I presume that, at some stage, there would be an isolation procedure that would remove the product from the leftover catalyst. I'd have to think about it to come up with a procedure such that SiCl4 or FeCl3 would be carried into the organic product but AlCl3 would be removed.
View user's profile View All Posts By User
sonogashira
National Hazard
****




Posts: 555
Registered: 10-9-2006
Member Is Offline

Mood: No Mood

[*] posted on 17-9-2006 at 11:53


Any idea how i would do this?.. what common solvents is AlCl3 soluble or insoluble in?
(by the way i am most certainly not making any drugs... i just happened to find that procedure using google.. not my fault if it happens to have "designer drugs" as a webpage!!)

Also, am i right in thinking that AlCl3 can be hydrolysed to Al(OH)3 which would be safe to ingest anyway?

(by the way matei, i am still interested in more info on that vogel reference if you have it... i haven't been able to find it as yet....)

[Edited on 17-9-2006 by sonogashira]
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 17-9-2006 at 12:09


Yes, but HCl isn't exactly safe. Plus lots of heat (see also CaCl2 MSDS). You get AlCl3 + 6H2O = AlCl3.6H2O followed by AlCl3 + 3H2O = Al(OH)3 + 3HCl (plus H2O of hydration).

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
The_Davster
A pnictogen
*******




Posts: 2861
Registered: 18-11-2003
Member Is Offline

Mood: .

[*] posted on 17-9-2006 at 12:14


http://www.sciencemadness.org/library/books/vogel_practical_...
;)
View user's profile View All Posts By User
sonogashira
National Hazard
****




Posts: 555
Registered: 10-9-2006
Member Is Offline

Mood: No Mood

[*] posted on 17-9-2006 at 12:59


Thanks a lot rogue chemist thats fantastic!!
Maybe i'm being slow but i cant find the AlCl3 sublimation procedure in this edition either... I've looked in the contents, index, and preparing inorganic solids but still cant find it....

Thanks for the link.. It seems even more useful than the 5th edition for my needs...
View user's profile View All Posts By User
matei
Hazard to Others
***




Posts: 205
Registered: 16-9-2006
Member Is Offline

Mood: No Mood

[*] posted on 21-9-2006 at 08:04


Sonogashira,

The purification procedure for AlCl3 is in Vogel's 5th Ed. on page 416.
I'm pretty sure AlCl3 is soluble in aromatic hydrocarbons (like benzene or toluene).
View user's profile View All Posts By User
sonogashira
National Hazard
****




Posts: 555
Registered: 10-9-2006
Member Is Offline

Mood: No Mood

[*] posted on 21-9-2006 at 17:02


Many thanks!!
View user's profile View All Posts By User
sonogashira
National Hazard
****




Posts: 555
Registered: 10-9-2006
Member Is Offline

Mood: No Mood

[*] posted on 15-10-2006 at 06:52


Does anyone know what solvents i can use with anhydrous aluminum chloride. i have seen a paper where they used 1,2-dichloroethane; would dichloromethane be ok, or would it react with it? Out of interest does anyone know why it doesn't react with 1,2-dichloroethane?
View user's profile View All Posts By User
 Pages:  1  

  Go To Top