Unlabelled jar with metal.
I have one unlabelled jar with granulated, dense metal... And I would like to figure out what is that metal... That metal chloride is soluble in water
- so it's isn't Lead. I think that is Zn or Sn. I found that Zn and Sn has pretty same properties ,but melting point of Sn is lower, but I can't
measure it right now. Can someone give me idea to figure out what is that metal and how... ?
On the right zinc :
http://img410.imageshack.us/my.php?image=comparemy7.jpg
Here is the bottle :
http://img410.imageshack.us/my.php?image=metaliq8.jpg
Grrrr.... Why ".jpg" forum shows like separate thing from that link ?! Just copy/paste in new window link. Thanks.
[Edited on 18-7-2006 by Maja]
|
|
chromium
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 284
Registered: 27-6-2005
Member Is Offline
Mood: reactive
|
|
Tin has so low melting point compared to Zn that you do not need thermometer to notice difference. For example pure tin will melt when touched with
soldering iron, droped to kitchen hotplate or held for a while in candle flame. It is still wise to make some additional tests as it may be some other
metal or alloy with low mp.
[Edited on 18-7-2006 by chromium]
|
|
The_Davster
A pnictogen
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2861
Registered: 18-11-2003
Member Is Offline
Mood: .
|
|
Zinc reacts with Dil HCl much faster than Sn. Ni2+, Co2+, Fe2+ will react with zinc but not tin.
|
|
Maja
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 143
Registered: 27-2-2006
Member Is Offline
Mood: No Mood
|
|
Quote: | Originally posted by chromium
Tin has so low melting point compared to Zn that you do not need thermometer to notice difference. For example pure tin will melt when touched with
soldering iron, droped to kitchen hotplate or held for a while in candle flame. It is still wise to make some additional tests as it may be some other
metal or alloy with low mp.
[Edited on 18-7-2006 by chromium] |
Yes, I will test it for melting... And I think that it's pure metal because it's from analytical lab, I do not think that they use alloys.
rogue chemist, thank you very much for that kind of information I will test it for Ni2+ ions tomorrow. Will report.
|
|
chemoleo
Biochemicus Energeticus
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline
Mood: crystalline
|
|
You could easily determine the density by the way. Just take a number of pellets, and put them in a measuring cylinder where water is in it to a
certain mark. Then weigh the dry pellets, and voila, the density.
If it is tin then you can do a quick test - take one pellet with two strong pliers, and bend it. If it is tin, it makes a screeching noise, which
results from the tin crystals being broken.
However, it is possible that some other metals do this too, but simply aren't so famous for it.
Never Stop to Begin, and Never Begin to Stop...
Tolerance is good. But not with the intolerant! (Wilhelm Busch)
|
|
YT2095
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
the first thing I`de try would be a magnet, that eliminates 4 metals, then a color test of the salts, a flame test for color or a borax bead test is
also good.
and as mentioned the all critical mass/volume test.
sometimes it`s worth getting a periodic table and making many photocopies of it, and using that as a Tick-Off list, to narrow the options down
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
AllanD
Harmless
Posts: 23
Registered: 16-7-2006
Member Is Offline
Mood: No Mood
|
|
I once found an unlabeled jar of granulated metal in the lab
when cleaning, my boss said "chuck it", So I did, into the "save for personal purposes" box....
I'm real glad I did, because as it turned out it was a bit over
100gms of Pt...
You say "dense" but don't say how dense.
Is it soft? Malleable?
are the granules shiny or dull?
Can they be pressed or formed into shiny bits?
Don't discount the possibility of it being Sb or
or metallic As (bad news)
AllanD
|
|
Brie
Harmless
Posts: 13
Registered: 3-6-2006
Member Is Offline
Mood: No Mood
|
|
Quote: | Originally posted by AllanD
I'm real glad I did, because as it turned out it was a bit over
100gms of Pt...
|
*whistles* ![:o](./images/smilies/shocked.gif)
yay for "acquiring" things like this...
Of course its always in the last place you look for it. What do you do, find something and keep looking?
|
|
Jdurg
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 220
Registered: 10-6-2006
Location: Connecticut, USA
Member Is Offline
Mood: No Mood
|
|
You can probably rule out arsenic because "metallic" Arsenic will tarnish VERY rapidly in open air into a dull grey, non-metal like mass.
\"A real fart is beefy, has a density greater than or equal to the air surrounding it, consists of the unmistakable scent of broccoli, and usually
requires wiping afterwards.\"
http://maddox.xmission.com.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
If you think its Sn or Zn, cast it into a bar, bend it and listen. Tin cries, zinc doesn't. (Sn isn't the only metal that does this but IIRC the
others have very low meilting points).
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Eh, zinc cries for me. I must be a depressing person... even annealed iron sometimes does (somewhat differently).
For that matter, last year when explaining "tin cry" in class... they used zinc rods...cheapasses!
Tim
|
|
IrC
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline
Mood: Discovering
|
|
I thought tin cried because it does not have a magnetic personality and cannot get women.
OK, crystal structure, blah blah blah.
|
|