Anhydroenneaheptitol pentanitrate?
This seems very intresting energetic material. Supposedly similar to PETN, little less sensitive and bit more brisant. It also needs not too exotic
chems (nor expensive) like acetone, formaline and Ca(OH)2 for anhydroenneaheptite and nitric acid to nitrate it (obviously, duh). There is old thread
on it at E&W forum http://www.roguesci.org/theforum/archive/index.php/t-111.htm... but no-one has reported any success making it. it seems there maybe little problem
getting crystallised anhydroenneaheptite but discussion stops there. I found it mentioned here too a few times but nothing useful. I also had a look
at PATR 2700 (vol1, A404) but it didnt give much details - On anhydroenneaheptitol - wh crystals (from alc) with mp 156.
On pentanitrate - 137% TNT, sensitivity in drop test with 2kg weight is 30 cm vs. 16 for PETN
PATR gives few refs though but I cant find these texts . is there particular reason
why its so unpopular? (It sounds good to me )
Does anyone have any related information on the subject or have someone tried to make it?
Thaks for help!
|
|
|
Rosco Bodine
Banned
Posts: 6370
Registered: 29-9-2004
Member Is Offline
Mood: analytical
|
|
The lack of interest is due to the low yield of the precursor synthesis which makes the process not cost effective in comparison to alternatives .
The fully nitrated product of maltitol ,
( having nine nitroester groups )
might be more interesting , in terms of ready availability of the precursor .
Inositol Hexanitrate is an even more interesting possibility , particularly if it has potential stability enhancement from a betaine stabilizer .
|
|
|
BASF
Hazard to Others
 
Posts: 282
Registered: 5-11-2002
Member Is Offline
Mood: hydrophilic
|
|
Newer synth...
This one is better.
A lot of work for a good yield though.
But...100% OTC
Exhaustive hydroxymethylation of acetone. Synthesis of anhydroenneaheptose. Olsen, Sigurd. Univ. Oslo, Norway. Chemische Berichte (1955),
88 205-12. CODEN: CHBEAM ISSN: 0009-2940. Journal language unavailable. CAN 49:42646 AN 1955:42646 CAPLUS
Abstract
Me, methylene, or methine groupings adjacent to the carbonyl in ketones can be exhaustively hydroxymethylated to 3,5-substituted
tetrahydro--pyrones. The reaction is illustrated on acetone. Tollens [Ber. 27, 1089(1894)] and Mannich (C.A. 17, 728) in condensing Me2CO
with HCHO in presence of CaO, obtained enneaheptitol and by dehydration anhydroheptitol (I). I is formed in greatly improved yield when the
condensation is carried out in HOAc-H2SO4. I has been recognized as 4-hydroxy-3,3,5,5-tetrakis(hydroxymethyl)tetrahydropyran. Paraformaldehyde(600
g.), 400 mL. HOAc, concd. 80 mL. H2SO4, and 40 mL. Me2CO are carefully mixed and then refluxed 3 h. The resulting dark red soln. is refluxed 1 h.
with 800 mL. 20% HCHO. The bis(methylene) ether (II) of anhydroenneaheptose is obtained on cooling; crystn. from 50% EtOH yields 235 g. colorless
crystals, m. 152, sapon. no. 0. The tetraacetate (III) of anhydroenneaheptose (32 g.), obtained by distg. 30 g. II with 200 mL. HOAc and 5
cc. concd. H2SO4, m. 101 (from EtOAc). Anhydroenneaheptose (IV) (12 g.) is obtained by hydrolysis of III (25 g.) with MeOH-HCl, m.
127. IV reduces Tollens soln., but does not react with carbonyl reagents. IV with Me2CO contg. HCl gives
bis(isopropylidene)anhydroenneaheptose, m. 19. The bis(methylene)ether of I, m. 222, has been prepd. by reducing II with HCHO in aq.
KOH and also by reducing II with Na in EtOH. Both were identical with the bis(methylene) ether prepd. by direct condensation of IV with HCHO. The
bis(methylene) ether of anhydroenneaheptitol monoacetate, m. 174; bis(anhydroenneaheptitol) triacetate, m. 106;
bis(anhydroenneaheptitol), m. 172.
    
[Edited on 17-10-2005 by BASF]
|
|
|
chemoleo
Biochemicus Energeticus
   
Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline
Mood: crystalline
|
|
Anhydro-enneaheptitol attempts
A long time ago I attempted to make some, and gleaned some insights from US patent 2885408 and the orgsyn prep for pentaerythritol.
I attempted several things, including using NaOH as a base.
The one attempt that produced a very syrupy, almost solid product (about 20 ml), that couldnt be concentrated further without decomposing (noticed by
a sugary smell and darkening of the colour).
Ba(OH)2 was used here.
I calculated the molar ratios from the patent, and adapted them here.
Preparation
A 1.4 molar excess of CH2O (in the form of paraformaldehyde) was used with respect to the acetone, when it is assumed that all is converted to the
final product.
Thus 100 g paraformaldehyde and 19.7 g acetone were mixed into 500 ml water.
To this suspension, 80.4 g of Ba(OH)2 *8H2O was added slowly. The temperature rises.
This was allowed to sit for 1 week at RT, with occasional shaking.
Then it was boiled down to 300 ml, filtered, and 25.0 g of H2SO4 (98%) was added to precipated the base as BaSO4. This was centrifuged/filtered,
it's a pain but figured that's the only way to get rid of the base. pH after neutralisation was 6.4, so it was all good. 
The final solution was boiled down to like 30 ml, until decomposition began. The syrup was initially clear until I overdid it and it started to
acquire a yellow/brown colour due to decomposition.
Tried to dissolve it in EtOH, to no avail, or dry it in ether, but dissolution wasn't really possible. Nonethelless, i think the water content of
the final product is very low, so one day this might be nitrated. Maybe someone else would like to try?
It certainly looked promising! If you look at the patent, the purification is not quite doable here.....
I also attempted the very same with 24% formaldehyde, and interestingly, this initial solution turned orange-red after day. Not sure what to make of
it, never followed it up further.
While with NaOH/24% formaldehyde, the solution remains clear, but also never followed that one up. Strange that the base would produce such a
difference.
Anyway, I definitley think there remains a lot of potential work to be done - reagents are cheap and accessible (at least more so that acetaldehyde in
the case of pentaerythritol).
[Edited on 17-10-2005 by chemoleo]
Never Stop to Begin, and Never Begin to Stop...
Tolerance is good. But not with the intolerant! (Wilhelm Busch)
|
|
|
Rosco Bodine
Banned
Posts: 6370
Registered: 29-9-2004
Member Is Offline
Mood: analytical
|
|
There are a couple of patents which are relevant to experiments with the reaction between acetone and formaldeyde , which can lead to several
different compounds .
GB361597
GB560669
These keto-polyols could perhaps be nitrated and also form peroxides at the carbonyl , or one or the other . If it was possible to do both nitration
and peroxidation , the result would be something like acetone peroxide dinitrate ,
and it possibly could cyclize as something like triacetone peroxide hexanitrate .
But I am skeptical about this being possible due to the vulnerability of the keto group to destructive oxidation .
Perhaps some scheme for protecting and then restoring the keto group would make the nitration and peroxidation possible . It is intriguing , since
the theoretical product would likely be a powerful explosive and very possibly a primary explosive .
Even in the absence of nitration or peroxidation , these materials have interest as binders , being polymerizable resins .
|
|
|
Axt
National Hazard
  
Posts: 973
Registered: 28-1-2003
Member Is Offline
Mood: No Mood
|
|
Appel, M. & Tollens, B. (1896)."<i>Ueber den Anhydro-ennea-heptit aus Formaldehyd und aceton</i>" Annalen der Chemie, 289,
46-51. [attached]
Attachment: Anhydroenneaheptitol.pdf (201kB) This file has been downloaded 1023 times
|
|
|
froot
Hazard to Others
 
Posts: 347
Registered: 23-10-2003
Location: South Africa
Member Is Offline
Mood: refluxed
|
|
This topic was touched on here in case it helps.
Since then I have tried the synth of the 'heptitol' using 1 unit weight acetone, 8 units of paraformaldehyde in a small amount of water. The
paraformaldehyde didn't completely dissolve but eventually disappeared in the duration of the reaction. I then continuously added CaOH every day
until the PH remained below 8.
After about a week the solution was boiled down to a syrup that reeked of formaldehyde. I then filled it up with hot water again and repeated the
boiling a couple of times in a feeble attempt to get rid of the formaldehyde. The temperature never went much above 100deg C.
I was drawn away from this experiment and 5 months later it is a thick greenish yellow syrup, no crystals. No smell of formaldehyde.
I'm sure there are still traces of Calcium in the sauce and don't think it will have a drastic effect on nitration, which I reckon it's
ready for.
My concern now is how to ensure complete nitration. I was thinking of a 2 stage nitration because the syrup still has water in it. Firstly using 60%
sulphuric and 55% nitric hoping for a precipitate which will then undergo a nitration as per PETN. If this is not the way to go for nitration then any
ideas on what would be?
We salute the improvement of the human genome by honoring those who remove themselves from it.
Of necessity, this honor is generally bestowed posthumously. - www.darwinawards.com
|
|
|
Helium
Harmless
Posts: 3
Registered: 15-10-2005
Member Is Offline
Mood: No Mood
|
|
Thaks for input guys!
dear BASF, do you have the whole text. It does use more chemicals and isnt maybe practical but just for sakes of chemical curiousity.
chemelo, that patent looks very interesting. I have some n-butyl acetate (at least I think I have - found it from old farm and loand some ). Is there an any easy way to "convert" it to n-butanol? Then I could
maybe try that purification step as described in patent.
Axt, that text looks like worth to read, too bad I cant speak german . I am
getting little pissed off by myself now not choosing germany as my second foreign language in school, because there are probably many more great texts
out there that would be very interesting to read 
| Quote: | originally posted by froot
My concern now is how to ensure complete nitration. I was thinking of a 2 stage nitration because the syrup still has water in it. Firstly using 60%
sulphuric and 55% nitric hoping for a precipitate which will then undergo a nitration as per PETN. If this is not the way to go for nitration then any
ideas on what would be?
|
I am really quessing here but precipitating the lower nitrated stuff from watery syrup might not work as desired.
Quoted From nitrated sugars thread
| Quote: | originally posted by PHILOU Zrealone at 8-9-2002 at 19:59
The only problem is to know if it is well nitrated or not...you can have a mix of 5 mononitrates esters+ 10 dinitrate esters+ 10 trinitrate ester + 5
tetranitrate esters and 1 pentanitrate ester...owing to the high probability of uncomplete nitration in non water free excess HNO3; the resulting
product might be hard to cristallise (owing to the mix of various molecules), hygroscopic (due to free OH unnitrated)
|
And anhydroenneaheptitols OHs seem to be very hydroscopic.
maybe some good desiccating agent helps to do the final job, dehydrating that damn syrupy anhydroenneaheptite. like CaCl2 - would be easyer an cheaper too 
Apparently there is also patent on that pentanitrate witch I would like read (to see how well it nitrates) but cant find. At E&W they give gb
28657 (1913) but in PATR gb 856,527 (1913), nether will give any results (at least not at http://v3.espacenet.com)
Well, I´ll do some experiments myself if I get the chance and see what happens.
|
|
|
Rosco Bodine
Banned
Posts: 6370
Registered: 29-9-2004
Member Is Offline
Mood: analytical
|
|
That patent is German , probably indexed as DRP286527 or perhaps less likely using a DE prefix .
|
|
|
BASF
Hazard to Others
 
Posts: 282
Registered: 5-11-2002
Member Is Offline
Mood: hydrophilic
|
|
| Quote: |
dear BASF, do you have the whole text. It does use more chemicals and isnt maybe practical but just for sakes of chemical curiousity.
|
In my opinion, the included method of using glacial acetic acid/H2SO4 gives a substantially improved yield and purity and is more likely be able to
prevent the trouble with the syrup. I think the syrupy consistency in the tollens´method is rather a consequence of impurities than of
hygroscopicity.
I´d not waste time with the historical tollens´method waiting months or so for the syrup to crystallize on porous dishes
Ok, the aforementioned method uses lots of precious glacial acetic acid, maybe there is a way of recycling it...
I have to look up the library for the "Chemische Berichte", to find out wether there is more information.
[Edited on 20-10-2005 by BASF]
[Edited on 20-10-2005 by BASF]
|
|
|
Axt
National Hazard
  
Posts: 973
Registered: 28-1-2003
Member Is Offline
Mood: No Mood
|
|
| Quote: | Originally posted by BASF
waiting months or so for the syrup to crystallize on porous dishes
|
Is that how it was isolated!, I couldnt read it either.
Let us know if you <i>dont</i> have luck getting the "ber" article, as I should be able to get it if needed.
BTW, if no one has drawn the connection there is ketone-formaldehyde condensation products mentioned in COPAE pg 285. Based on cyclopentanone and
cyclohexanone, which forms castable nitration products of simular structure to the anhydroenneaheptitol.
|
|
|
Rosco Bodine
Banned
Posts: 6370
Registered: 29-9-2004
Member Is Offline
Mood: analytical
|
|
The Von Herz patent DE286527 is attached
Attachment: DE286527 Anhydroenneaheptite Pentanitrate.pdf (138kB) This file has been downloaded 927 times
|
|
|
Helium
Harmless
Posts: 3
Registered: 15-10-2005
Member Is Offline
Mood: No Mood
|
|
| Quote: | originally posted by BASF
I think the syrupy consistency in the tollens´method is rather a consequence of impurities than of hygroscopicity.
|
If you are correct it sounds quite good actually. I alaways thought that its the hygroscopicity of AhE that f***s things up and that it decoposes
before all water could evaporate when heating. Both tollens and olsen method produce aqueous solution of AhE, if I am correct, unless dry HCl is used
in olsens (" Anhydroenneaheptose (IV) (12 g.) is obtained by hydrolysis
of III (25 g.) with MeOH-HCl," . So I figured that those other methods would be
better. But lot of things are still unclear here! (to me at least )
I am looking fovard of your findings at library!.
|
|
|
BASF
Hazard to Others
 
Posts: 282
Registered: 5-11-2002
Member Is Offline
Mood: hydrophilic
|
|
Translation of the first part(the second concerns analysis of the anhydroenneaheptite)
XLVI. About the anhydro-enneaheptite from formaldehyde and aceton 
from Dr.M.Apel and B.Tollens
1. Preparation and Properties(not included)
Some years ago Dr. F. Mayer obtained, by bringing acetone, formaldehyde, lime and water together, removal of the lime(not CaCO3 but CaO) with oxalic
acid and boiling to dryness, a syrup, in which the one of us after two years found several crystals.
This caused us to bring the abovementioned materials together again, to possibly obtain more of the mentioned crystals.
60g acetone, 240g formaldehyde(600g 40% solution), 6000g water, 65g previously prepared milky dispersion of lime (Ca(OH)2 here) was left stood in a
bigger flask for a long time - up to 4 weeks- under repeated shaking.
In later preparations the flask was left stood at a 35°C warm place.
Subsequently, the flask with the mixture was heated in a boiling water-bath for some time, the liquid was decanted from the settled solid and filtered
and freed from the lime, still boiling, by accurate precipitation with oxalic acid(ca. 115g).
The filtrates were concentrated to the syrup under stirring in the water bath.
These syrups crystallized upon seeding with the previously obtained substance, therefor they had become crystal pulps after 8 or 10 days, but
sometimes the crystallization took weeks and months using exactly the same preparation method and was less complete.
Treatment of the syrup with alcohol and ether, through which a part was dissolved, another part stayed undissolved, offered no advantage, because the
obtained fractions at good products (?) crystallized both, at not easily crystallizing products both yielded hardly any crystals.
As good as possible crystallized pulps were brought onto porous dishes made of clay and yielded dark, sometimes nearly white, dry, sometimes dark soft
products, which had to be applied onto new dishes repeatedly.
The crystals were then dissolved in few water or alcohol and dissolved by heating, upon which they crystallized better and faster; multiple
recrystallization with activated charcoal from alcohol completed the purification.
(...)
[Edited on 21-10-2005 by BASF]
|
|
|
BASF
Hazard to Others
 
Posts: 282
Registered: 5-11-2002
Member Is Offline
Mood: hydrophilic
|
|
Here it is. Thanks to myself for typing ...
I decided not to leave out the introduction, because it refers to the drawbacks of the tollens´method compared to olsens´ procedure.
32. Sigurd Olsen: About the exhaustive oxymethylation of acetone. Synthesis of an anhydro-ennea-heptose
(...)
The condensation of acetone with formaldehyde in excess in the presence of calcium hydroxide was conducted by B.Tollens and coworkers for the first
time, who managed the isolation of the substance C9H18O6 with the MP 156°C during very time-consuming work.
(...)
Later it was repeatedly tried to oxymethylate aceton with numerous alkaline condensation-agents in polycondensation-conditions, but these attempts as
well as the attempts of J.R.Roach, H.Wittcoff and S.E.Miller ("per"oxymethylation coupled with alkylation) are only of peripheral
interest, as they show the possibility of partial oxymethylation in alkaline medium -thus generally under tollens´reaction conditions- without
simultaneous reduction of the carbonyl group (...)
Such a simultaneous reduction can act already against the starting material itself as well as against all intermediates to the
"per"oxymethylation final product, and prevents further condensation with formaldehyde by the formation of alcohols.
The formation of the "per"methylation-product would then only be possible with the few molecules escaping the hydrogenating side-reaction.
Under these sircumstances a very complex mixture of substances is generated by the tollens´reaction, which would serve as a satisfying explanation
for the formation of the "crystallization-lame" syrups described by tollens and other authors, on the other hand also gives an explanation
for the bad yields and the difficult isolation of the reduced "per"oxymethylation product.
Maybe this is the reason why the tollens´reaction was not able to establish itself as preparative method.
The biggest disadvantage of the tollens´reaction is the difficult to conduct reduction in the last phase, in which the carbonyl group of the
"per"oxymethylation product is reduced to the carbinol group by reagent in excess, which causes the replacement of the precious
ß-keto-alcohol of sugar-character by the less precious correspondent multi-valent alcohol.
In some cases it was managed to catch the "per"oxymethylation-product before the reduction by the application of stoicheometric amounts of
formaldehyde 4)
(C.Mannich and W.Brose and others); still these methods are considered inferior (...)
The abovementioned drawbacks of the tollens´reaction now are obsolete when using glacial acetic acid /sulfuric acid instead of alkaline solution.
(note of the authors: This cannot strictly be considered an acid catalyzed reaction, because it fails without addition of glacial acetic acid when
only using aqueous sulfuric acid alone)
(...) no reduction of the carbonyl group occurs under these conditions, even when formaldehyde is in excess.
(...)
The advantages of the condensation in glacial acetic acid/sulfuric acid as opposed to alkaline condensation are as follows:
1.)short reaction time
2.)no undesired side-reactions
3.)ease of isolation of the non-reduced "per"oxymethylation-product
4.)its easily and seperately conducted reduction to the corresponding alcohol
Preparation:
1.exhaustive hydroxymethylation of acetone in glacial acetic acid/sulfuric acid:
A mixture of 600g paraformaldehyde, 400ml glacial acetic acid, 80ml conc. sulfuric acid and 140ml pure acetone was heated carefully til the beginning
of the reaction.
When the reaction subsided, the mixture was boiled 3 hours under reflux. The dark red liquid then was mixed with 800ml 20% formalin solution and
boiled for 1 hour for the saponification of acetates. After cooling down colourless needles crystallized and where vacuum filtered and recrystallized
from 50% ethanol. yield: 235g; MP 152°C
Bismethylene ether of anhydro-ennea-heptose (VI)
C11H16O6 (244,2)
2. Tetraacetate of anhydro-enneaheptose (V):
30g of (VI) was distilled with 200ml glacial acetic acid and 5ml sulfuric acid under dropwise addition of glacial acetic acid, taking care to keep a
constant volume of liquid in the flask.
After 500ml distillate have gone over, no formaldehyde could be observed using 2,4-diphenylhydrazine/HCl.
After cooling down, water was added to the flask. Yield was 32g of a light brown substance, which got colourless after recrystallization from ethyl
acetate and melted at 101°C.
C17H24O10(388,4)
3.Anhydro-enneahepatose (IV):
25g of the above described tetraacetate yielded after reesterification with methanolic hydrochloric acid and redissolving from ethyl acetate 12g of a
completely colorless substance of sweet taste, which reduces tollens´solution, melts at 127°C and is unreactive with carbonyl-reagents.
C9H16O6(220,1)
That´s it..... i deserve a break right now....

[Edited on 22-10-2005 by BASF]
|
|
|
Axt
National Hazard
  
Posts: 973
Registered: 28-1-2003
Member Is Offline
Mood: No Mood
|
|
Thanks for the translation BASF, its appreciated. For a nitrate the synth looks a bit nasty for me considering I have more acetaldehyde then I'll
ever need.
I did end up getting the article, so I might as well attach it.
[Edited on 28-10-2005 by Axt]
Attachment: Anhydroenneaheptitol-2.pdf (581kB) This file has been downloaded 1191 times
|
|
|
BASF
Hazard to Others
 
Posts: 282
Registered: 5-11-2002
Member Is Offline
Mood: hydrophilic
|
|
Thanks for the scan Axt .
Here the translation of the one important part i really did not want to miss. ... the synth is comprehensive only to the anhydro-anneaheptose, which
is only the precursor to anhydro-anneaheptite. forgive me ...
Anhydro-enneaheptite(II):
20g Anhydro-enneaheptose were dissolved in 100ml hot formalin and 50g cryst. barium hydroxide in 100ml water were added within a few minutes, which
caused the solution to react vigorously under boiling.
The liquid reacted neutral to litmus and, but still had a strong formaline-smell and was boiled a further 10mins, filtered hot and boiled nearly to
dryness.
As this residue still had a smell of formaldehyde, a solution of 10g sodium hydrogensulfite in 40ml water was added and the reaction mixture was
boiled til a sticky mixture of salt resulted.
After thoroughly mixing ("verreiben" "anreiben" what does it equal in english??) with anhydrous sodium sulfate it was extracted 6
hours with 300ml dry ethyl acetate in a soxhlet extractor(i hate this part, further complicating a complicated procedure).
In the extraction big quantities of a colorless substance already solidified.
After vacuum filtration(better transl for "absaugen", anyone?) 17g of the abovementioned substance of MP 135-146°C were obtained. The MP
did not vary much after recrystallization from various different solvents.
The substance did not reduce Tollens´ solution, thus the contained impurity cannot be the starting material. For save identification, a sample of the
substance was taken up with a small quantity of warm ethanol, then acetone and a few drops of HCl were added and heated for a moment to dissolve the
substance. Upon cooling a big quantity of colorless lamella ("blättchen"
crystallized, sharp MP at 230°C and gave no melting point lowering with bis-isopropylideneether (p.a. purity).
[Edited on 29-10-2005 by BASF]