I thought about it today at work, and I was thinking i liked the idea of just disolving the rods HCl. Since AgCl is insoluble and every thing else
just stays in solution. The only thing is where to go once I have silver chloride? Is there an easy way to convert it into silver nitrate? I would
much rather have silver nitrate than silver chloride.
N/A
|
|
|
neutrino
International Hazard
   
Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline
Mood: oscillating
|
|
The silver shouldn't be attacked, providing you exclude oxygen from the acid.
|
|
|
tom haggen
Hazard to Others
 
Posts: 488
Registered: 29-11-2003
Location: PNW
Member Is Offline
Mood: a better mood
|
|
What about using aqua regia?
N/A
|
|
|
Fleaker
International Hazard
   
Posts: 1254
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
Aqua regia will give you silver chloride, it impedes further chemical action. It's a common problem with high silver alloys and why gold refiners
dilute the alloy with copper: makes it easier for the silver to go into soln.
|
|
|
tom haggen
Hazard to Others
 
Posts: 488
Registered: 29-11-2003
Location: PNW
Member Is Offline
Mood: a better mood
|
|
so since the alloy I have is such a low percentage of silver, no silver chloride will precipitate?
N/A
|
|
|
Fleaker
International Hazard
   
Posts: 1254
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
At 5% silver, you might still have problems with silver chloride buildup on the outside of the metal that is being digested. I suggest melting it and
shotting it (to get rid of phosphorus by melting in an oxidizing atmosphere). Then dissolvein nitric acid which will put everything into solution
assuming it's just copper, silver, palladium, and less noble base fillers.
Do you know the exact composition of the alloy?
|
|
|
Mr. Wizard
International Hazard
   
Posts: 1042
Registered: 30-3-2003
Member Is Offline
Mood: No Mood
|
|
I just checked ebay, and the sil-phos silver solder is going for &12.50 a pound plus $4 shipping. Why mess with purifying it? Sell it and save
yourself the trouble. If you just want silver you can buy it with the profits. A happy solution ;-)
|
|
|
Fleaker
International Hazard
   
Posts: 1254
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
I agree, you can make a lot more money by selling it for what it is than by refining it.
|
|
|
Ephoton
Hazard to Others
 
Posts: 463
Registered: 21-7-2005
Member Is Offline
Mood: trying to figure out why I need a dark room retreat when I live in a forest of wattle.
|
|
yep
aqua disolve watch out for the no2 gas.
if you dont get any gas its not working.
make aqua from one part nitric acid to 3 parts hydrochloric.
once disolved distill multiple time but never to dryness by adding hydrochloric acid when nearly dry.
once all nitric is gone dilute with water
then percipitate with your choice of reducing agent (ferrous ion, oxalic or formic acid, sulfites and so2, metalic zinc
ect ect)
collect your gold and wish you lived in oz near a reef
|
|
|
Ephoton
Hazard to Others
 
Posts: 463
Registered: 21-7-2005
Member Is Offline
Mood: trying to figure out why I need a dark room retreat when I live in a forest of wattle.
|
|
now other metals
if you want the plat group out of a solution it gets harder.
you must be more selective of your reducing agents.
first a oxalic acid drop is my choice then
ammonium chloride to get the group.
fire up the group then redisolve in clean
aqua.
oxidize solution to put palladium in a different oxidation state than platinium.
drop Pt with ammonium chloride. then
make solution basic with ammonia to drop
Pd 
if you want silver buy a braclet
Os and others are realy hard and require
molten alkali disolves (realy nasty)
|
|
|
Ephoton
Hazard to Others
 
Posts: 463
Registered: 21-7-2005
Member Is Offline
Mood: trying to figure out why I need a dark room retreat when I live in a forest of wattle.
|
|
silver
silver will not disolve in aqua but it will disolve in nitric acid.
if you do an aqua disolve and find white powder at the bottom of you flask you could possibly have silver.
|
|
|